Reversible oxidation of WOx and MoOx nano phases
International audience; WOx and MoOx nano phases were prepared on TiO2(1 1 0) surfaces by a CVD procedure consisting of adsorption and decomposition of W(CO)(6) or Mo(CO)(6) precursors followed by annealing under UHV. Metal amount involved in each elaborated sample is in the fractional range from 0.1 to 0.35 equivalent monolayer (eqML) of W or Mo. Evolution of sample stoichiometry as a function of subsequent treatment is followed by valence band and core level photoemission as well as work function measurement. In each case, exposure of samples to molecular oxygen at room temperature induces an increase of sample work function in a range of several tenth of eV. Such a work function change i…