THERMOTROPIC HOMOPOLYESTERS. IV. STUDY OF FIBER FORMATION.
We report a melt spinning and viscosity study of two semiflexible homopolyesters containing both rigid and flexible segments in the repeating unit. Single filaments of the polyesters formed from 4,4′-diacetoxybiphenyl and azelaic acid (PB7) and sebacic acid (PB8), and from 4′-hydroxyphenyl-4-hydroxycinnamate and azelaic acid (C7), were spun at temperatures between 205 and 255°C. The temperature dependence of the Newtonian melt viscosity of PB7 and C7 was investigated, and a range of molecular weights was studied for PB7. The spinning parameters, fiber characteristics, and viscosity-temperature behavior are related to the type of mesophase formed. The mechanical properties of fibers spun fro…