0000000000714899
AUTHOR
Pouran Samimi
showing 1 related works from this author
Interfacial fracture toughness of universal adhesive systems treated with an antioxidant
2017
Background Secondary caries, degradation of the dentin-resin interface and fracture of the restoration are the most common forms of failure. The aim of this study was to assess the interfacial fracture toughness of three different adhesive approaches and to compare their fracture toughness after surface treatment with antioxidant. Material and methods Seventy two dentin blocks with 3×4mm dimension and 3mm thickness were prepared and attached to precured 3×4×12mm composite blocks from both sides. Six adhesive groups (N=12), All-bond universal, Scotchbond universal and Clearfil SE bond with or without antioxidant treatment (Sodium Ascorbate 10% )were applied to dentin surfaces, a 160µ polyeth…