Comparative fracture behavior of monolithic and veneered zirconia posterior fixed dental prostheses

2017

The purpose of this study was to evaluate and to compare the fracture load and the fracture pattern of monolithic and veneered zirconia posterior fixed dental prostheses (FDPs). Twenty standardized steel dies were prepared to receive posterior 3-unit FDPs. Specimens were randomly divided into 2 groups (n=10): (1) Lava Zirconia, and (2) Lava Plus. All FDPs were cemented using glass ionomer cement and subjected to thermal and mechanical cycling at 5-55ºC with a 30-s dwell time for 120,000 masticatory cycles. All specimens were subjected to a three-point bending test until fracture. Data were statistically analyzed using Student's t test, paired t-test and Weibull statistics (α=0.05). No diffe…

Dental Stress AnalysisMaterials scienceGlass ionomer cementDentistryDental Abutments02 engineering and technologyBendingVeneering ceramicDental Materials03 medical and health sciences0302 clinical medicineMaterials TestingCubic zirconiaDental Restoration FailureGeneral Dentistrybusiness.industryFracture loadMonolithic zirconia030206 dentistryStainless Steel021001 nanoscience & nanotechnologyDental VeneersGlass Ionomer CementsCeramics and CompositesFracture (geology)Computer-Aided DesignDenture Partial FixedZirconium0210 nano-technologybusinessDental Materials Journal
researchProduct

Effect of Thermomechanical and Static Loading on the Load to Fracture of Metal‐Ceramic, Monolithic and Veneered Zirconia Posterior Fixed Partial Dent…

2018

PURPOSE To evaluate the influence of static (not preloaded) and thermomechanical loading on the load to fracture of metal-ceramic, monolithic and veneered zirconia computer-aided design/computer-aided manufacturing (CAD/CAM) posterior fixed partial dentures (FPDs). MATERIALS AND METHODS One hundred standardized specimens with 2 abutments screwed onto a platform were prepared from stainless steel to receive a posterior 3-unit FPD with an intermediate pontic. Specimens were randomly divided into 5 groups (n = 20): Metal-ceramic (control group), Lava Zirconia system, Vita In-Ceram YZ, IPS e.max ZirCAD, and Lava Plus. Half of the specimens of each group (n = 10) underwent no preloading, and the…

Dental Stress AnalysisMaterials scienceMetal Ceramic AlloysDental Abutments02 engineering and technologyCrossheadDental MaterialsRandom Allocation03 medical and health sciences0302 clinical medicineMaterials TestingFixed partial denturesCubic zirconiaDental Restoration FailureComposite materialGeneral DentistryUniversal testing machineFracture loadMonolithic zirconia030206 dentistryStainless Steel021001 nanoscience & nanotechnologyMetal ceramicDental VeneersFracture (geology)Computer-Aided DesignDenture Partial FixedStress MechanicalZirconium0210 nano-technologyJournal of Prosthodontics
researchProduct

Disinclusion of unerupted teeth by mean of self-ligating brackets: Effect of blood contamination on shear bond strength

2012

Objectives: The aim of this study was to assess the effect of blood contamination on the shear bond strength and failure site of three different orthodontic self-ligating brackets. Study Design: 240 bovine permanent mandibular incisors were randomly divided into 12 groups of 20 specimens each. Orthodontic self-ligating brackets were tested under four different enamel surface conditions: a) dry, b) blood contamination before priming, c) blood contamination after priming, d) blood contamination before and after priming. Brackets were bonded to the teeth and subsequently tested using a Instron universal testing machine. Shear bond strength values and adhesive failure rate were recorded. Statis…

Dental Stress AnalysisMaterials scienceOrthodontic BracketsBlood contaminationDentistryOdontologíaOrthodonticsDental bondingstomatognathic systemShear strengthAnimalsTooth UneruptedGeneral DentistryOrthodonticsUniversal testing machineEnamel paintBond strengthbusiness.industryDental Bonding:CIENCIAS MÉDICAS [UNESCO]Ciencias de la saludShear bondstomatognathic diseasesBloodOtorhinolaryngologyvisual_artUNESCO::CIENCIAS MÉDICASvisual_art.visual_art_mediumCattleResearch-ArticleSurgeryAdhesiveShear StrengthbusinessMedicina Oral Patología Oral y Cirugia Bucal
researchProduct

Retentive strengths of cast gold crowns using glass ionomer, compomer, or resin cement

1998

The retention forces of a newly developed compomer cement (Dyract Cem), a glass ionomer cement (Ketac Cem Aplicap), and a resin cement (F21) were examined.Cemented cast gold crowns were removed along the path of insertion with a Zwick universal testing device. The impact of both a cured and a noncured additional bonding layer that were applied to the inner surface of the crowns was examined across the Dyract Cem group.The mean adhesive strength was measured at 2.36 +/- 0.69 N/mm2 in the Ketac Cem group, at 0.60 +/- 0.28 N/mm2 in the F21 group, and at 1.85 +/- 0.94 N/mm2 in the Dyract Cem group, respectively. The application of an additional bonding layer to the inner surface of the crowns d…

Dental Stress AnalysisMaterials scienceSurface PropertiesPolyestersGlass ionomer cementDental CementsComposite ResinsDental Prosthesis RetentionAdhesion strengthHumansComposite materialCementationResin cementCementPolycarboxylate CementCrownsCompomersSilicatesDental BondingAdhesivenessResin CementsDyract-cemGlass Ionomer CementsDentinGold AlloysMethacrylatesStress MechanicalZinc OxideOral SurgeryMagnesium OxideThe Journal of Prosthetic Dentistry
researchProduct

Influence of prefabricated post dimensions on restored maxillary central incisors

2007

summary  The aim of this study was to test the following hypothesis: biomechanical performance (fracture strength and stress distribution) of restored teeth is less sensitive to post diameter and post length when using glass fibre posts than when using stainless steel posts. First, an experimental fracture strength test was performed on 80 extracted human maxillary central incisors. Teeth were decoronated, treated endodontically and restored (40 with glass fibre posts and 40 with stainless steel posts), and the length and diameter of the posts varied uniformly. Failure loads were recorded and results were compared using an ancova analysis. Secondly, the finite element technique was used to …

Dental Stress AnalysisMaterials sciencebusiness.industryFinite Element AnalysisGlass fiberDentistryModels TheoreticalStress distributionStainless SteelModels DentalIncisorDental MaterialsDental Prosthesis DesignFlexural strengthMaterials TestingHumansComputer SimulationMaxillary central incisorDental Restoration FailureGlassFinite element techniquebusinessGeneral DentistryPost and Core TechniqueJournal of Oral Rehabilitation
researchProduct

In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents

2005

Statement of problem In contrast to gold crowns, in vitro determination of the retentive strength of all-ceramic crowns is more difficult because components allowing connection to testing apparatus are not as easily integrated into the all-ceramic material. Nevertheless, retentive strength data are crucial for obtaining information about the potential clinical performance of luting cements for all-ceramic restorations. Therefore, a new in vitro model was necessary to evaluate the retentive strength of all-ceramic crowns. Purpose The purpose of this in vitro study was to determine the retentive strength of 4 resin-cement systems, a compomer, a glass-ionomer cement, a resin-modified glass-ion…

Dental Stress AnalysisMaterials sciencemedicine.medical_treatmentDental CementsDentistryCrown (dentistry)Dental Prosthesis RetentionDental porcelainstomatognathic systemDental cementMaterials TestingmedicineHumansCeramicComposite materialCementationCementUniversal testing machineCrownsCompomersbusiness.industryLuting agentEpoxyDental PorcelainResin CementsGlass Ionomer Cementsvisual_artvisual_art.visual_art_mediumZirconiumOral SurgerybusinessThe Journal of Prosthetic Dentistry
researchProduct

Premolars restored with posts of different materials: fatigue analysis

2011

Previous works studied the effect of the material and the dimensions of the post on the biomechanical performance (fracture strength and stress distribution) of restored teeth, under static loads. The aim of this work was to study the effect of the post material (glass fibre and stainless steel) on restored teeth, which have the final crown, under dynamic conditions. The use of a biomechanical model, including a fatigue analysis from FEA, is presented as a powerful method to study the effect of the material of the intraradicular post. The inclusion of the fatigue analysis allows for a more realistic study that takes into account the dynamic nature of masticatory forces. At the same time, th…

Dental Stress AnalysisMaterials sciencemedicine.medical_treatmentGlass fiberInfluence of post materialMaterials testingCrown (dentistry)Bite ForceDental MaterialsTooth FracturesFlexural strengthMaterials TestingmedicineHumansImplant denturesBicuspidComposite materialGeneral DentistryFEAFatigueTooth NonvitalCrownsImplants dentalsRestored teethStress distributionStainless SteelFinite element methodDental Prosthesis DesignDental Stress AnalysisCeramics and CompositesBiomechanical modelGlassDental materials--FatiguePrefabricated intraradicular postsMaterials dentals--FatigaDental AlloysPost and Core Technique
researchProduct

Primary loading of palatal implants for orthodontic anchorage--a pilot animal study.

2006

Summary Objectives This study aimed at evaluating the clinical performance and osseointegration of short orthodontic implants immediately loaded with orthodontic forces. Material and methods The investigation was designed as an experimental animal study. Eight palatal implants of the Ortho-system® were immediately loaded with 100 cN after palatal insertion in 4 female german shepherd dogs. Xylene orange and calcein green were used for polychrome sequential labelling. Histological preparation utilized the cutting and grinding technique. Outcome variables were clinical implant success, histological osseointegration and bone-to-implant contact rates. Results All (8/8) implants were clinically …

Dental Stress AnalysisPalate HardTime FactorsDentistryPilot ProjectsDevice implantOsseointegrationDogsImplants ExperimentalOsseointegrationOrthodontic Anchorage ProceduresMedicineAnimalsAnimal studyBone formationbusiness.industryClinical performanceAppositionBone to implant contactOtorhinolaryngologyMicroscopy FluorescenceSurgeryFemaleImplantOral SurgerybusinessJournal of cranio-maxillo-facial surgery : official publication of the European Association for Cranio-Maxillo-Facial Surgery
researchProduct

Luting of ceramic crowns with a self-adhesive cement: Effect of contamination on marginal adaptation and fracture strength

2012

Objectives: This study evaluated the percentages of continuous margins (%CM) and fracture strength (FS) of crowns made out from blocs of leucite-reinforced ceramic (IPS Empress CAD) and luted with a representative self-adhesive cement (RelyX Unicem) under four contaminating agents: saliva, water, blood, a haemostatic solution containing aluminium chloride (pH= 0.8) and a control group with no contamination. Study Design: %CM at both tooth-cement (TC) and cement-crown (CC) interfaces were determined before and after a fatigue test consisting of 600’000 chewing loads and 1’500 temperature cycles changing from 5º C to 50º C. Load to fracture was recorded on fatigued specimens. Kruskal-Wallis t…

Dental Stress AnalysisSalivaAluminium chlorideDental CementsDentistryOdontologíaIn Vitro TechniquesDental porcelainFlexural strengthDental cementBiomaterials and Bioengineering in DentistryDentinmedicineHumansGeneral DentistryCementCrownsChemistrybusiness.industryContamination:CIENCIAS MÉDICAS [UNESCO]Dental PorcelainCiencias de la saludddc:617.6Resin Cementsmedicine.anatomical_structureOtorhinolaryngologyUNESCO::CIENCIAS MÉDICASResearch-ArticleSurgerybusinessmedicine.drugMedicina Oral Patología Oral y Cirugia Bucal
researchProduct

Fracture resistance after implantoplasty in three implant-abutment connection designs

2020

Background To assess the effect of implantoplasty and implant-abutment design on the fracture resistance and macroscopic morphology of narrow-diameter (3.5 mm) dental implants. Material and Methods Screw-shaped titanium dental implants (n = 48) were studied in vitro. Three groups (n = 16) were established, based on implant-abutment connection type: external hexagon, internal hexagon and conical. Eight implants from each group were subjected to an implantoplasty procedure; the remaining 8 implants served as controls. Implant wall thickness was recorded. All samples were subjected to a static strength test. Results The mean wall thickness reductions varied between 106.46 and 153.75 µm. The me…

Dental Stress AnalysisTitanium implantMaterials scienceCirurgia dentalchemistry.chemical_elementDental Abutments03 medical and health sciences0302 clinical medicineFlexural strengthDental AbutmentsMaterials TestingGeneral DentistryEndosseous dental implantsDental ImplantsTitaniumOrthodonticsCrownsResearchConnection (principal bundle)030206 dentistry:CIENCIAS MÉDICAS [UNESCO]OtorhinolaryngologychemistryDental surgeryUNESCO::CIENCIAS MÉDICASFracture (geology)SurgeryImplants dentals intraossisImplantImplantologyImplant abutmentTitanium
researchProduct