Dentin bonding agent with improved bond strength to dentin through incorporation of sepiolite nanoparticles.

2017

Background The study aims to investigate the effect of incorporation of sepiolite nanoparticles on the microtensile bond strength of an experimental dentin bonding to the human dentin. Material and methods The sepiolite nanoparticles were incorporated into an experimental methacrylate-based dentin bonding system in concentrations of 0.0, 0.2, 1.0, 2.0, and 5.0 weight percents. The specimens were then ultrasonicated to finely disperse the nanoparticles in the adhesive matrix. The coronal enamel of 30 intact human premolars was cut to expose dentin. Having etched, rinsed, and blot dried the experimental bonding agents were applied to dentin surface. Adper Single Bond was used as control group…

Materials scienceComposite numberDentistry02 engineering and technologyMethacrylateOperative Dentistry and Endodontics03 medical and health sciences0302 clinical medicinestomatognathic systemDentinmedicineSingle bondComposite materialGeneral DentistryEnamel paintBond strengthbusiness.industrySepioliteResearch030206 dentistry021001 nanoscience & nanotechnology:CIENCIAS MÉDICAS [UNESCO]stomatognathic diseasesmedicine.anatomical_structurevisual_artUNESCO::CIENCIAS MÉDICASvisual_art.visual_art_mediumAdhesive0210 nano-technologybusinessJournal of clinical and experimental dentistry
researchProduct

Evaluating the shear bond strength of enamel and dentin with or without etching: a comparative study between dimethacrylate-based and silorane-based …

2015

Background: Silorane-based composites and their specific self-etch adhesive were introduced to conquest the polymerization shrinkage of methacrylate-based composites. It has been shown that additional etching of enamel and dentin can improve the bond strength of self-etch methacrylate-based adhesives but this claim is not apparent about silorane-based adhesives. Our objective was to compare the shear bond strength (SBS) of enamel and dentin between silorane-based adhesive resin and a methacrylate-based resin with or without additional etching. Material and Methods: 40 sound human premolars were prepared and divided into two groups: 1- Filtek P60 composite and Clearfil SE Bond adhesive; 2- F…

Materials scienceComposite numberDentistryOdontologíaMethacrylateOperative Dentistry and Endodonticsstomatognathic systemEtching (microfabrication)DentinmedicineComposite materialGeneral DentistryShrinkageEnamel paintBond strengthbusiness.industryResearchtechnology industry and agriculture:CIENCIAS MÉDICAS [UNESCO]Ciencias de la saludstomatognathic diseasesmedicine.anatomical_structurevisual_artUNESCO::CIENCIAS MÉDICASvisual_art.visual_art_mediumAdhesivebusiness
researchProduct

Bulk filling of Class II cavities with a dual-cure composite: Effect of curing mode and enamel etching on marginal adaptation.

2014

Objectives: This study attempted to find a simple adhesive restorative technique for class I and II cavities on posterior teeth. Study Design: The tested materials were a self-etching adhesive (Parabond, Coltene/Whaledent) and a dual-cure composite (Paracore, Coltene/Whaledent) used in bulk to restore the cavities. Class II MO cavities were performed and assigned to 4 groups depending on the orthophosphoric acid (H3PO4) conditioning of enamel and polymerization method used (chemical or dual). Specimens were subjected to quantitative marginal analysis before and after thermo-mechanical loading. Results: Higher percentages of marginal adaptation at the total margin length, both before and aft…

Materials scienceComposite numberDentistryOdontologíaOperative Dentistry and Endodonticschemistry.chemical_compoundstomatognathic systemEtching (microfabrication)DentinmedicineComposite materialGeneral DentistryPhosphoric acidCuring (chemistry)Enamel paintbusiness.industryResearch:CIENCIAS MÉDICAS [UNESCO]Ciencias de la saludddc:617.6stomatognathic diseasesmedicine.anatomical_structurechemistryvisual_artUNESCO::CIENCIAS MÉDICASPosterior teethvisual_art.visual_art_mediumAdhesivebusinessJournal of clinical and experimental dentistry
researchProduct

Effect of bleaching agents on sealing properties of different intraorifice barriers and root filling materials

2012

Objective: To evaluate the effect of intracoronal bleaching agents on the sealing properties of different intraorifice barriers and root filling materials. Study Design: The root canals of extracted human premolars (n=180) were prepared by using System GT rotary files and filled with either gutta-percha+AH Plus or Resilon+Epiphany sealer. In both groups, the coronal 3mm of root filling was removed and replaced with one of the following materials applied as intraorifice barriers (n=30/group): 1. ProProot-MTA; 2. Conventional Glass ionomer cement; and 3. Hybrid resin composite. In each subgroup, intracoronal bleaching was performed using either sodium perborate with distilled water or 35% hyd…

Materials scienceGlass ionomer cementDentistryEndodonticsRoot Canal Filling MaterialsBleaching Agentschemistry.chemical_compoundMaterials TestingRoot fillingHumansBicuspidComposite materialHydrogen peroxideFluid filtrationGeneral DentistryLeakage (electronics)Dental Leakagebusiness.industry:CIENCIAS MÉDICAS [UNESCO]Epiphany sealerOtorhinolaryngologychemistryDistilled waterUNESCO::CIENCIAS MÉDICASResearch-ArticleSurgerySodium perboratebusiness
researchProduct

The effect of oxalate-based desensitizers on the microleakage and shear bond strength of resin modified glass ionomer

2017

Background The first line of intervention to alleviate tooth sensitivity is to use dentin desensitizers such as oxalate-based desensitizers. When the dentin sensitivity continues even after application of desensitizers the next intervention would be restoration of the lesion. The aim of this in vitro study was to investigate the effect of prior application of oxalate-based desensitizer on the marginal microleakage and shear bond strength of resin modified glass ionomer (RMGI) restorations. Material and methods In order to prepare the specimens for microleakage test standard class v cavities were prepared on buccal surfaces of 45 teeth. The specimens were randomly divided into three equal gr…

Materials scienceGlass ionomer cementDentistryOxalateOperative Dentistry and Endodontics03 medical and health scienceschemistry.chemical_compound0302 clinical medicinestomatognathic systemStereo microscopeDentinmedicine030212 general & internal medicineGeneral DentistryDentin SensitivityEnamel paintbusiness.industryResearch030206 dentistry:CIENCIAS MÉDICAS [UNESCO]medicine.diseasestomatognathic diseasesmedicine.anatomical_structurechemistryvisual_artTooth SensitivityUNESCO::CIENCIAS MÉDICASvisual_art.visual_art_mediumDentin hypersensitivitybusinessJournal of Clinical and Experimental Dentistry
researchProduct

The effect of different insertion techniques on the depth of cure and vickers surface micro-hardness of two bulk-fill resin composite materials

2016

BACKGROUND The aim of this study was to evaluate the Vickers surface micro-hardness and the depth of cure of two bulk-fill resin composites and one incremental-fill resin composite. MATERIAL AND METHODS Two Bulk-fill dental resin composites (X-tra Fil, Voco; Sonic-FillTM 2, Kerr Corporation) and an incremental-fill dental resin composite (Filtek™ Z250 XT, 3M ESPE) were used. Sixty cylindrical specimens of 4 mm thickness were prepared using split Teflon moulds. Specimens were divided into six groups (n=10) according to the type of the material used and according to the insertion technique applied (bulk or incremental). Prepared specimens were stored dry in complete darkness at 37°C for 24 ho…

Materials scienceHardness ratioResin compositeResearchSignificant differenceBulk fillOdontología030206 dentistry02 engineering and technology:CIENCIAS MÉDICAS [UNESCO]021001 nanoscience & nanotechnologyIndentation hardnessCiencias de la saludOperative Dentistry and Endodontics03 medical and health sciences0302 clinical medicineUNESCO::CIENCIAS MÉDICASDental resin compositeComposite material0210 nano-technologyGeneral Dentistry
researchProduct

Bond strength of dental nanocomposites repaired with a bulkfill composite

2017

Background The aim of this study was to analyze the bond strength of aged resin based nanocomposites repaired with the same and bulk fill composites. Material and Methods Seventy-two disc shaped resin composites consisted of three different nanocomposite resins (Filtek Ultimate/FU, Herculite XRV Ultra/HXRV, and Reflectys/R) were produced. After storing the samples for 8 weeks in distilled water, each material was combined with the same material or the bulk-fill composite resin system (Filtek Ultimate+Filtek Ultimate/Group-1; Filtek Ultimate+Tetric BF/Group-2; Herculite XRV+Herculite XRV/Group-3; Herculite XRV+Tetric BF/ Group-4; Reflectys+Reflectys/Group 5; Reflectys+Tetric BF/Group-6), for…

Materials scienceNanocompositeBond strengthResearchResin compositeComposite numberSignificant differenceBulk fill030206 dentistry02 engineering and technology:CIENCIAS MÉDICAS [UNESCO]021001 nanoscience & nanotechnologyOperative Dentistry and Endodontics03 medical and health sciences0302 clinical medicineHerculite XRVUNESCO::CIENCIAS MÉDICASAdhesiveComposite material0210 nano-technologyGeneral DentistryJournal of Clinical and Experimental Dentistry
researchProduct

Fracture resistance of tooth restored with four glass fiber post systems of varying surface geometries-An in vitro study

2016

Background The purpose of this study was to relate the fracture resistance of endodontically treated teeth in relation to post geometry. Material and methods Forty single rooted mandibular premolars were instrumented by step - back technique and obturated by lateral condensation. Forty teeth were randomly divided into four groups: Reforpost glass fiber X-ray®, RelyX®, Exacto conical® and Parapost Fiber Lux®. The post spaces were prepared using respective drills and luted. The core build up was done and metal crowns were luted. Fracture resistance was determined in universal testing machine. The statistical analysis was done using one way ANOVA and post hoc Tukey Kramer test. Results The tee…

Materials sciencePost hoc0206 medical engineeringGlass fiberDentistryOdontología02 engineering and technologyLateral condensationOperative Dentistry and Endodontics03 medical and health sciences0302 clinical medicinestomatognathic systemIn vitro studyStatistical analysisGeneral DentistryUniversal testing machinebusiness.industryParallel designResearch030206 dentistry:CIENCIAS MÉDICAS [UNESCO]020601 biomedical engineeringCiencias de la saludstomatognathic diseasesUNESCO::CIENCIAS MÉDICASFracture (geology)businessJournal of Clinical and Experimental Dentistry
researchProduct

Effect of different polishing techniques on surface roughness and bacterial adhesion of three glass ionomer-based restorative materials : in vitro st…

2020

Background Although many reports concluded that polishing of glass ionomers is crucial for smoother surface and limiting the adhesion of cariogenic bacteria, there is no specific surface treatment protocol recommended. A novel material in the same category was released recently claimed to have surface smoothness comparable to resin composite and bacterial adhesion less than other types of glass ionomers. In this study, different polishing systems were tested with three glass ionomers one of them is the novel material to find the most appropriate polishing protocol. Objectives: To evaluate and compare the surface roughness and bacterial adhesion to resin modified glass ionomer, bioactive ion…

Materials sciencePost hocResearch0206 medical engineeringGlass ionomer cementPolishing030206 dentistry02 engineering and technology:CIENCIAS MÉDICAS [UNESCO]020601 biomedical engineeringPaint adhesion testingGloss (optics)Operative Dentistry and Endodontics03 medical and health sciences0302 clinical medicineUNESCO::CIENCIAS MÉDICASSurface roughnessIn vitro studyComposite materialACTIVA BioACTIVE-RESTORATIVEGeneral Dentistry
researchProduct

Intensity output and effectiveness of light curing units in dental offices

2018

Background The aims of the study were measuring the light intensity of light curing units used in Qazvin's dental offices, determining the relationship between the clinical age of these units and their light intensity, and identifying the reasons for repairing them. Material and Methods In this cross-sectional study, the output intensity of 95 light curing devices was evaluated using a radiometer. The average output intensity was divided up into four categories (less than 200, 200-299, 300-500, and more than 500 mW/cm2). In addition, a questionnaire was designed to obtain information mainly about the type, clinical age, and frequency of maintenance of the units and the reasons for fixing th…

Materials scienceResearch030206 dentistry02 engineering and technology:CIENCIAS MÉDICAS [UNESCO]021001 nanoscience & nanotechnologylaw.inventionIntensity (physics)Operative Dentistry and EndodonticsLight curing03 medical and health sciencesLight intensity0302 clinical medicineDental OfficeslawUNESCO::CIENCIAS MÉDICASNegative correlation0210 nano-technologyGeneral DentistryLight-emitting diodeBiomedical engineeringJournal of Clinical and Experimental Dentistry