Shear bond strength and debonding characteristics of metal and ceramic brackets bonded with conventional acid-etch and self-etch primer systems: an i…
2016
Background: Different in-vitro studies have reported various results regarding shear bond strength (SBS) of orthodontic brackets when SEP technique is compared to conventional system. This in-vivo study was designed to compare the effect of conventional acid-etching and self-etching primer adhesive (SEP) systems on SBS and debonding characteristics of metal and ceramic orthodontic brackets. Material and Methods: 120 intact first maxillary and mandibular premolars of 30 orthodontic patients were selected and bonded with metal and ceramic brackets using conventional acid-etch or self-etch primer system. The bonded brackets were incorporated into the wire during the study period to simulate th…
Effect of saliva contamination on bracket failure with a self-etching primer: A prospective controlled clinical trial
2010
Introduction The aim of this study was to evaluate in vivo the effect of saliva contamination at different stages of the bonding procedure on the bond failure rate and the adhesive remaining on teeth after debonding brackets bonded with a hydrophilic self-etching primer (Transbond Plus self-etching primer [TSEP], 3M Unitek, Monrovia, Calif). Methods This was a prospective controlled clinical trial. The sample consisted of 46 patients with similar treatment plans and mechanotherapies. Stainless steel brackets (n = 531) were bonded with TSEP. The patients were divided into 2 groups: contamination with saliva before TSEP application and contamination with saliva after TSEP application. In both…
Resistance to demineralisation of adjacent enamel and dentine, fluoride release and dentine bond strength of fluoride-containing self-etch adhesive s…
2019
Background The current study aimed to assess the amount of fluoride released from fluoride-containing dental adhesives and its effect on micro-tensile bond strength (µTBS) and on resistance to demineralisation of dentine and enamel. Material and Methods Two fluoride-containing dental adhesives, and a fluoride-free adhesive were used as experimental adhesives. After thermal cycling the µ-TBS of adhesives to dentine and the failure mode were assessed. The fluoride release and cross-sectional microhardness (CSMH) of specimens were measured before and after one day, 7 and 28 days of pH-cycling. The data were analysed using one-way ANOVA, Weibull statistics and repeated measures ANOVA. Results T…
POSITIONING SELF-ETCHING ADHESIVES: VERSUS OR IN ADDITION TO PHOSPHORIC ACID ETCHING?
2004
In vitro bond strengths post thermal and fatigue load cycling of sapphire brackets bonded with self-etch primer and evaluation of enamel damage
2020
Background This in vitro study compares a self-etch primer (SEP) to an etch-and-rinse (EaR) for bonding sapphire brackets by evaluation of the enamel etch-pattern, shear bond strength, amount of remnant adhesive and enamel surface damage following thermal and fatigue cyclic loading. Material and Methods Ceramic (sapphire) brackets were bonded to 80 extracted human premolars using two enamel etching protocols: conventional EaR using 37% phosphoric acid (PA) gel (control), and a SEP (Transbond Plus). Each group was subdivided into two subgroups (n=20 teeth) according to the time of bracket debonding: after 24 h water storage or following 5000 thermo-cycles plus 5000 cycles fatigue loading, to…
Comparative evaluation of sealing ability, penetration and adaptation of a self etching pit and fissure sealant- stereomicroscopic and scanning elect…
2019
Background The efficacy of pit and fissure sealants in preventing occlusal caries is a well-established fact. Considering the difficulty in achieving strict isolation for a longer duration while treating the pediatric patients, a simplified procedure of sealant application is desirable. While, a self-etching sealant, Prevent Seal offers a quick procedure, the physical properties of this material haven’t been studied yet. Thus, this study was aimed to comparatively evaluate sealing ability, penetration and adaptation of a self-etching pit and fissure sealant and a conventional resin sealant. Material and Methods This was an in vitrointergroup comparative study, which consisted of 2 groups- G…
Effect of Chlorhexidine on durability of two self-etch adhesive systems
2020
Background Despite of the rapid development in the field of dental adhesives, the issue of reduction in dentin bond durability has still not been resolved. The activity of dentinal endogenous enzymes such as MMPs is one of the most important causes of failure in resin composite restorations. The aim of this study was to investigate the influence of Chlorhexidine on micro-tensile bond strength of two types of commercially available self-etch adhesives. Material and Methods Twenty four sound and freshly extracted molars were selected. Four standardized flat mid-coronal dentinal disks were prepared from each tooth. The specimens were randomly assigned to 6 groups (n=16). Groups A(control group…
Effect of a plant-based hemostatic agent on microleakage of self-etching adhesives
2012
Objective: This in vitro study evaluated the effect of Ankaferd Blood Stopper (ABS) contamination on the micro-leakage of one-step and two-step self-etching adhesives.
Evaluation of the enamel etching pattern of self-etching adhesives
2010
Objectives: To evaluate the capacity of seven self-etching adhesives (SEAs) to demineralize ground enamel in comparison with traditional phosphoric acid etchant (PAE) using SEM and statistical analysis. Materials and methods: 80 caries-free extracted human third molars were divided into 8 groups ( n = 10). Enamel bur-cut surfaces were prepared and, strictly following the manufacturers’ instructions, treated with three priming agents of two-step self-etching adhesives: Aqua Resulcin Prime (Group 1); Peak™ (Group 2); Clearfil Protect Bond (Group 3); four one-step self-etch (all-in-one) adhesives, G-Bond (Group 4); Artegral One (Group 5); Clearfil S3 Bond (Group 6); Adper Easy Bond (Group 7); …
Marginal quality of a full-body bulk-fill composite placed with an universal adhesive system in etch-and-rinse and self-etch mode: An
2020
Background Marginal seal of a nanohybrid bulk-fill composite compared to a nanohybrid conventional composite, using a universal adhesive (UA) applied in etch-and-rinse (ER) and self-etch (SE) mode was investigated. Material and Methods Thirty-six intact molars were selected and two standardized cavities in each tooth were prepared and allocated into four groups according to restorative material and etching strategy. All samples were placed in a 1% methylene blue solution for 24 h, then cut in the middle of the restorations obtaining two parts (n=144) and used for microscopic evaluation (50x) for dye penetration measurements. Results The data were analysed by ANOVA and Tukey post-hoc test (p…