Fracture strength of endodontically treated lateral incisors restored with new zirconia reinforced rice husk nanohybrid composite
2020
Background This study aimed to compare the fracture strength, fracture pattern and type of fracture of endodontically treated maxillary lateral incisors restored with new zirconia reinforced rice husk nanohybrid composite. Material and Methods Eighty mature permanent maxillary lateral incisors from patients age range of 30-60 years with single canal were selected and randomly divided into: Group 1 – RCT + nanofilled composite (Filtek), Group 2 – RCT + microhybrid composite (Zmack), Group 3 – RCT + new nanohybrid composite (Zr-Hybrid) and Group 4 - Intact teeth (control). Standardized mesio-palatal-distal cavity was prepared, and endodontic treatment was carried out using crown-down techniqu…
Experimental strength of restorations with fibre posts at different stages, with and without using a simulated ligament
2011
The aim of this study was to analyse the strength and failure mode of teeth restored with fibre posts under retention and flexural-compressive loads at different stages of the restoration and to analyse whether including a simulated ligament in the experimental setup has any effect on the strength or the failure mode. Thirty human maxillary central incisors were distributed in three different groups to be restored with simulation of different restoration stages (1: only post, 2: post and core, 3: post-core and crown), using Rebilda fibre posts. The specimens were inserted in resin blocks and loaded by means of a universal testing machine until failure under tension (stage 1) and 50o flexion…
The effect of orthodontic bracket pad shape on shear bond strength, an in vitro study on human enamel
2018
Background To evaluate the effect of bracket pad shape on shear bond strength (SBS) of orthodontic brackets bonded to human enamel. Material and Methods One hundred and five extracted human maxillary permanent molars were divided into 7 groups of 15 specimens per group (n=15). Each group of teeth was bonded with 6 different shaped WildSmiles® brackets (Star, Heart, Soccer ball, Football, Flower, and Diamond) and GAC® rectangle shaped brackets. Shear debonding force was measured with an Instron universal testing machine using a knife-edged chisel 24 hours after initial bonding. Descriptive statistics (mean, standard deviation, and range) for each bracket pad shape was calculated. Analysis of…
Photoelastic analysis of conventional and locking system for treatment of mandibular angle fractures with a single plate
2021
Made available in DSpace on 2021-06-25T10:28:10Z (GMT). No. of bitstreams: 0 Previous issue date: 2021-04-01 Background: This photoelastic analysis evaluated stress distribution in different osteosynthesis systems, conventional and locking, used for treatment of mandibular angle fractures with a single plate. Material and Methods: Angle fractures were simulated in mandibles made of photoelastic resin. Following Champy’s method, plate osteosynthesis was performed. The samples were divided into five groups: Group 1, non-fractured mandible; Group 2, two screws were installed in each segment using a conventional system; Group 3, two screws were installed in each segment using a locking system; …
Comparison of torque expression in esthetic brackets
2019
Background The objective of this work is to test the null hypothesis that there is no difference in the torque expression among different esthetic brackets. Material and methods Five ceramic self-ligating brackets (In-Ovation C - GAC, Damon Clear-Ormco, QuicKlear-Forestadent, Click-It -TP Orthodontics, Clarity SL-3M Unitek) and 4 ceramic conventional brackets (Inspire Ice-Ormco, InVu Ceramic-TP Orthodontics, Ceramic Roth-Morelli, Clarity Metal-Reinforced Ceramic Bracket-3M Unitek) were selected. Metallic Damon MX self-ligating bracket (Ormco) was used as control. Third-order moments were measured at 12o, 24o and 36o using an archwire torsion device associated with a Universal Testing Machin…
The effect of dental chair light exposure duration on shear bond strength of orthodontic brackets : an in vitro study
2018
Background The purpose of this study is to determine if the duration of exposure to the halogen overhead dental chair light has an effect on shear bond strength (SBS) of metal orthodontic brackets. Material and Methods One hundred twenty extracted human lower incisor teeth were divided into six groups (n=20/group). Each group was assigned a predetermined duration of exposure to the halogen dental chair light, set at a fixed distance, before being cured. Light exposure times of 0 minutes (Group 1-Control), 1 minute (Group 2), 2.5 minutes (Group 3), 5 minutes (Group 4), 10 minutes (Group 5), and 15 minutes (Group 6) were tested. Each tooth was subjected to an exclusion criteria examination, s…
Influence of low concentration acid treatment on lithium disilicate core/veneer ceramic bond strength
2013
Objective: This study evaluated the influence of low concentration acid treatment on the shear bond strength between lithium disilicate (LD) infrastructure and veneering porcelain. The surface morphology characteristic after this acid treatment was also examined. Study Design: LD reinforced ceramic cylinders (n=10) (IPS e.max Press, Ivoclar-Vivadent, Schaan, Liechtenstein) were treated (LD-treated) with a low concentration acid solution (Invex Liquid – Ivoclar-Vivadent, Schaan, Liechtenstein) or not treated with the acid solution (LD-untreated). They were veneered with a glass ceramic (IPS e.max Ceram, Ivoclar-Vivadent, Schaan, Liechtenstein). A metal ceramic group (CoCr) was tested as cont…
Comparison between different surface treatment methods on shear bond strength of zirconia (in vitro study)
2020
Background To compare the effect of Er:YAG Laser and Air particle abrasion (APA) surface treatments on shear bond strength of Y-TZP to composite resin cuboids in the presence and absence of primer application and salivary contamination. Material and methods Seventy-two cuboidal shaped specimens 7x7x3 were prepared from Y-TZP using CADCAM, cleaned and sintered. Specimens were divided into 2 main groups (n=36) according to surface treatment method; Air particle abrasion (A) and laser (L). Each group was subdivided into 2 subgroups (N = 18) according to surface modification using primer; each subgroup was further divided into 2 subdivisions (N=9) according to the presence of salivary contamina…
Shear bond strength of ceramic fused to CAD-CAM milled alloys
2018
Background This study evaluated the metal ceramic bond strength of cast Ni-Cr, cast Co-Cr, sintered Co-Cr and milled Co-Cr alloys to ceramic through two application procedures including the ceramic layering technique and ceramic pressed-on technique. Material and Methods Ceramic materials (Ø 8 mm, 1.5 mm thickness) were veneered by either the layering or pressed-on technique to cast Ni-Cr, cast Co-Cr, sintered Co-Cr and hard milled Co-Cr alloy disc (12 × 12 × 0.5 mm) (n=15). All specimens were treated with a thermal cycle process for 500 cycles at the temperature between 5 °C and 55 °C with immerse time of 30 seconds and 5 seconds for specimen transfer. The shear bond strength was determine…
Post-fatigue fracture resistance of metal core crowns: press-on metal ceramic versus a conventional veneering system
2014
Background The aim of this in vitro study was to compare the mechanical failure behavior and to analyze fracture characteristics of metal ceramic crowns with two veneering systems – press-on metal (PoM) ceramic versus a conventional veneering system – subjected to static compressive loading. Material and Methods Forty-six crowns were constructed and divided into two groups according to porcelain veneer manufacture. Group A: 23 metal copings with porcelain IPS-InLine veneering (conventional metal ceramic). Group B: 23 metal copings with IPS-InLine PoM veneering porcelain. After 120,000 fatigue cycles, the crowns were axially loaded to the moment of fracture with a universal testing machine. …