Search results for "titanium alloy"
showing 10 items of 86 documents
Evaluation of Residual Stresses During Fatigue Test in an FSW Joint
2008
At present, friction stir welding (FSW) represents one of the most interesting techniques in the field of welding. The process is has been implemented in industrial practice for joining aluminium alloys, while the welding of the titanium alloy and the steels is still primarily in a developmental stage.
Fatigue Crack Growth in Titanium and Aluminium Alloys under Bending
2007
The paper contains results of investigations of the crack growth in plane specimens made of Ti-6Al-4V titanium alloy and AlCu4Mg1 aluminium alloy under cyclic bending. The tests were done on specimens with the stress concentrators being one-sided sharp notch. On the fractures there have been observed first of all transcrystalline cracks through the α phase grains for both materials.
Optimisation of TA6V alloy surface laser texturing using an experimental design approach
2008
International audience; Active surfaces of plastic injection moulds are nowadays textured using classical techniques (chemical etching or EDM). Replacement of these technologies by a laser technology introduces a big flexibility: absence of mechanical contact with the tool, decrease of the effluent's volume and a big machining precision, even in the case of the complex forms as injection moulds for example. This paper reports the experimental study of the surface laser texturing of TA6V alloy. The influence of the operating factors on the laser texturing process has been studied using two experimental approaches: Taguchi methodology and response surface methodology (RSM). Empirical models h…
Corrosion Behaviour of Ti6Al4V and TiMo10Zr4 Alloys in the Ringer’s Solution: Effect of pH and Plastic Strain
2015
The corrosion behaviour of titanium alloys is not well understood – especially the role of the microstructure and plastic strain. In this paper, the influence of the microstructure and plastic strain on the corrosion resistance of TiMo10Zr4 and Ti6Al4V alloys was studied in the Ringer’s solution at 37 °C. Measurements were performed for different pH values and in aerated and de-aerated solutions using potentiodynamic polarization techniques. Results obtained on the two alloys were compared. It was shown that in the absence of plastic strain TiMo10Zr4 shows better corrosion resistance than Ti6Al4V (especially for pH = 8). By contrast, the current density in the passive range measured after 8…
The Effect of Building Direction on Microstructure and Microhardness during Selective Laser Melting of Ti6Al4V Titanium Alloy
2021
AbstractDuring the last few years, additive manufacturing has been more and more extensively used in several industries, especially in the aerospace and medical device fields, to produce Ti6Al4V titanium alloy parts. During the Selective Laser Melting (SLM) process, the heterogeneity of finished product is strictly connected to the scan strategies and the building direction. An optimal managing of the latter parameters allows to better control and defines the final mechanical and metallurgical properties of parts. Acting on the building direction it is also possible to optimize the critical support structure. In particular, more support structures are needed for the sample at 0°, while very…
Cell and tissue response to nanotextured Ti6Al4V and Zr implants using high-speed femtosecond laser-induced periodic surface structures
2019
In this paper, the effect of femtosecond laser nanotexturing of surfaces of Ti6Al4V and Zr implants on their biological compatibility is presented and discussed. Highly regular and homogeneous nanostructures with sub-micrometer period were imprinted on implant surfaces. Surfaces were morphologically and chemically investigated by SEM and XPS. HDFa cell lines were used for toxicity and cell viability tests, and subcutaneous implantation was applied to characterize tissue response. HDFa proliferation and in vivo experiments evidenced the strong influence of the surface topography compared to the effect of the surface elemental composition (metal or alloy). The effect of protein adsorption fro…
Use of pure vanadium and niobium/copper inserts for laser welding of titanium to stainless steel
2020
Abstract Niobium and vanadium have high metallurgical compatibility with titanium and therefore can be used as inserts to avoid the accumulation of brittle intermetallic phases such as Fe2Ti during the fusion welding of titanium alloys with steels. In the present study, the continuous double pass welding of 1 mm thick Ti-6Al-4V alloy and 316 L stainless steel plates through several mm wide pure vanadium or niobium insert was studied. In case of a vanadium insert, a beam offset on the vanadium was found to produce cold crack formation in vanadium/316 L melted zones containing more than 40 wt.% V despite the absence of σ phase. Whereas a centered beam position and offset on the steel side pro…
Sample building orientation effect on porosity and mechanical properties in Selective Laser Melting of Ti6Al4V titanium alloy
2022
Abstract In recent decades, the focus of research has shifted towards new production technologies with the aim of optimizing production and reducing costs. These innovative technologies include additive manufacturing processes as Selective Laser Melting (SLM). The analysis of the literature on the identification of optimal building orientation to maximize the mechanical properties and minimize porosity of the final products highlights contrasting results, denoting that the thermomechanical complexity of the process, as associated with the variation of the building orientation, has not been fully clarified. A study in which the building orientation effect was evaluated together with the geom…
Thermal effects of continuous laser treatment on Ti-6 Al(wt%)-4V(wt%) titanium alloy
2008
A titanium alloy Ti-6 Al(wt%)-4V(wt%) was treated in air by Nd:YAG laser radiation (wavelength of 1.064 %m) in continuous mode. Targets were irradiated globally with different levels of energy (accumulated fluence) at constant power. Different focal lengths and beam displacement velocities were used. Cross section microstructural observations were carried out by scanning electron microscopy. Backscattered electron imaging reveals microstructural modifications in samples. A structural phase transformation of beta (bcc) to alpha prime (hcp) phase was observed. The depth of the transformed zone observed by phase transformation is dependent on the treatment parameters. Conformity between micros…
Interactions between cells and titanium surfaces.
2002
The interaction between cells and implant materials is determined by the surface structure and/or surface composition of the material. In the past years, titanium and titanium alloys have proved their superiority over other implant materials in many clinical applications. This predominant behaviour is caused by a dense passive oxide layer which forms within milliseconds in oxidizing media. Titanium dioxide layers of 100 nm thickness were produced on the surface of cp-titanium grade 2, and on an experimental alloy of high vanadium content (Ti1.5Al25V) as a harmful control. The layers were produced by thermal and anodic oxidation and by coating by means of the sol-gel process. The resulting o…