The effect of prolonged storage time on asphalt rubber binder properties
2019
Abstract This study wants to provide fundamental understanding of prolonged storage time on asphalt rubber binder properties by performing an investigation on the variation of conventional properties, rheology and morphology of four asphalt rubbers maintained at 180 °C in low shear for different digestion/storage times up to 48 h. The analysed asphalt rubbers were manufactured by combining two different asphalt binder grades, pen 35/50 and pen 50/70, with both cryogenic and ambient crumb rubber. Results have shown that keeping asphalt rubber agitated at the above mentioned processing conditions, up to 48 h, is significantly detrimental when an ambient crumb rubber is used, while it seems no…
Fatigue and Healing Properties of Low Environmental Impact Rubberized Bitumen for Asphalt Pavement
2017
The addition of recycled tyre rubber as a modifier to enhance the mechanical properties of bitumen has proven to provide asphalt mixtures with better mechanical performance. However the rubberised bitumen presents the limitation of requiring higher manufacturing and compaction temperatures. This could be solved by subjecting the tyre rubber to sort of pre-treatments such as: Adding warm-mix additives and/or using partial devulcanisation. These solutions have the potential of lowering the overall environmental impact of the asphalt pavement, however it is still not clear whether these can be detrimental for the rubberized asphalt binder mechanical properties. This paper investigates the effe…
Micromechanisms of load transfer in a unidirectional carbon fibre–reinforced epoxy composite due to fibre failures. Part 1: Micromechanisms and 3D an…
2006
This study gives a detailed analysis of load distributions around fibre breaks in a composite and the mechanisms involved in load transfer. In contrast to other studies reported in the literature the analysis considers different configurations of composite damage from the failure of a few fibres to the failure of many. The model considers the elastic case with and without debonding at the broken fibre/matrix interface. In this way, the usual limitations of the finite element approach are overcome so as to take into account the numbers and interactions of broken fibres whilst maintaining an evaluation of the various fields involved, in particular the stress fields associated with fibre failu…
Influence of cation order on the dielectric properties of (1 – x)Pb(Sc 0:5 Nb 0:5 )O 3 -xPb(Yb 0:5 Nb 0:5 )O 3 ceramics
2020
Ceramic lead niobates and their solid solutions (1 - x)Pb(Sc0:5Nb0:5)O3 - xPb(Yb0:5Nb0:5)O3 were synthesized by solid state reactions from oxides. The structure of investigated samples was characterized by X-ray diffraction (XRD). Dielectric studies of the ceramics were performed by means of broadband dielectric spectroscopy at the temperature ranging from 600 K to 140 K. For all ceramic samples a diffuse phase transition as well as relaxor ferroelectric behavior were observed. © 2020 Barbara Garbarz-Glos et al., published by Sciendo 2020. This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License.
Adsorption of single Ag and Cu atoms on regular and defective MgO(001) substrates: an ab initio study
2004
Abstract The DFT slab calculations were performed for Ag and Cu atoms adsorbed on both regular and defective MgO(0 0 1) substrates. Both metal atoms and surface O vacancies ( F s centers) were distributed uniformly with a concentration of one Ag, Cu or F s per 2×2 surface supercell. Surface O 2− ions are energetically more preferable for metal-atom adsorption on a regular substrate as compared to Mg 2+ ions. The nature of the interaction between Ag or Cu adatoms and a defectless MgO substrate is physisorption (despite the difference in the adsorption energies: 0.62 vs. 0.39 eV per Cu and Ag adatom, respectively). Above the F s centers, metal atoms are bounded much stronger when compared wit…
Metal Matrix Composites - Mmc - Turning: Comparison of Tool Materials
2002
The main properties required to the modem cutting tools to be employed in production, are both high wear resistance and chemical stability. In this last years, in the machining of MMCs several kinds of coated tools have been developed; they are characterized by high hardness to resist to the relevant strength and abrasive action of the reinforce fibers or particles, arranged inside the matrix. In turning of MMC the employ of Tungsten Carbide tools coated with Polycrystalline Diamond (PCD) have shown to be very effective, whereas they are very expensive thus increasing the production costs.
Effects of powder concentration and type of resin on the performance of marble composite structures
2009
In this work, we will expose the behaviour of a composite structure reinforced with marble powder. The attention was focused on the effects produced on the physical and mechanical properties due to different kinds of matrix (epoxy and polyester resins) and filler amounts (60%, 70%, 80%). Rheological, static flexural and Izod impact tests have been carried out. An experiment designed was defined for the mechanical tests, in order to quantify the effects of both the resin and the marble percentage on the material properties, as well as to identify a possible correlation between these factors. Moreover, water absorption and stain resistance have been evaluated to study the surface properties o…
Fracture toughness of synthesised high-performance epoxies subject to accelerated water aging
2018
Abstract The effects of water uptake on the fracture toughness of epoxy systems with high glass-transition temperatures (Tg above 170 °C) are investigated. Aging conditioning has been conducted in hot water, followed by a desorption conditioning in a room temperature dry-airborne. Water aging determines plasticisation effects and crosslink-density modifications, revealed by reductions of the Tg. It is less known how such modifications influence the material fracture toughness. In this study, Single Edge Notched Bending samples have been tested according to standards, to evaluate the KIC fracture toughness at different stages of water absorption-desorption. The characterisation has been supp…
Moisture Absorption Effects on the Resistance to Interlaminar Fracture of Woven Glass/Epoxy Composite Laminates
2012
The influence of moisture absorption on the interlaminar fracture behaviour of 8/8 harness satin weave glass/epoxy composite was investigated. Two series of specimens with 0°/0° and 90°/90° predominant interfaces immersed in water for different duration were tested under double cantilever beam (DCB mode I), single leg bending (SLB mode I + II) and end notched flexural (ENF mode II) loadings. In general, the apparent flexural modulus: E, and the fracture toughness: G C, decrease with increasing moisture content. This effect is more remarkable if mode II participation is bigger. The value of G C measured on 90°/90° specimens reveals higher than that on 0°/0° ones, but the variation in G C is …
Carbon Fiber Composites Cured by γ-Radiation-Induced Polymerization of an Epoxy Resin Matrix
2008
The use of ionizing radiation in order to initiate polymerization of suitable monomers has found increased interest in the last two decades due to its several advantages. In this work, carbon fiber composites through gamma radiation polymerization of epoxy matrices have been produced for aerospace and advanced automotive applications. Composite samples were produced by irradiation at room temperature using different radiation doses and, as reference, thermal curing of the same epoxy resin formulations was also carried out. Furthermore, some irradiated samples were subjected to postirradiation thermal curing to complete the polymerization reactions. The properties of the cured materials were…