Highly trans-stereospecific Isoprene Polymerization by Neodymium Borohydrido Catalysts
Highly stereospecific polymerization of isoprene was achieved using borohydridoneodymium complexes. In combination with stoichiometric amounts of dialkylmagnesium, Nd(BH4)3(THF)3 (1) and Cp*‘Nd(BH4)2(THF)2 (2) (Cp*‘ = C5Me4nPr) afford very efficient catalysts. The activity reaches 37300 (g of polyisoprene/mol of Nd)/h. Half-lanthanidocene 2 gives rise to polyisoprene, 98.5% trans-regular, the highest content yet described for a homogeneous organometallic catalyst. NMR experiments argue for the formation of bimetallic Nd(μ-BH4)Mg active species.