Polarization of SrBi 2 Ta 2 O 9 ceramics at infra‐low frequencies
Dielectric response in the SrBi2Ta2O9 ceramics is studied over a wide range of temperatures at fields up to Emax ≈ 18 kV/cm. Dependence of dielectric permittivity on field intensity is analyzed at different temperatures. A series of polarization loops are obtained at frequencies 0.1 Hz, 1 Hz, and 10 Hz. The hysteresis at switching polarization is displayed by the shape of polarization loops changing with the field amplitude from bi-angles to quasi-saturated loop patterns of a high degree of rectangularity. The ratio of remnant polarization to maximum polarization as function of field amplitude is presented. Thermal behaviour of the coercive field and the half-width of polarization loops is …