In vitro experimental study of bonding between aluminium oxide ceramics and resin cements

2010

To evaluate bond strengths of different resin cements to two aluminum oxide-based ceramics. Methods: One hundred ten ceramic cylinders were produced and given four different surface treatments. Resin cement cylinders were then bonded to the ceramic cylinders using different resin cements and the bond strength was determined by shear testing to the breaking point. We were thus able to obtain results for the different combinations of porcelain, surface treatments and cements. All data was analyzed using the Kruskal-Wallis test for more than two independent samples and the Bonferroni correction applied (a=0.01). An optical microscopy study was carried out to analyze the type of failure, and an…

CeramicsMaterials scienceDental bondinglaw.inventionchemistry.chemical_compoundOptical microscopelawMaterials TestingAluminum OxideCeramicComposite materialGeneral DentistryAluminum oxideCementBond strengthDental Bonding:CIENCIAS MÉDICAS [UNESCO]SilicateResin CementsOtorhinolaryngologychemistryvisual_artUNESCO::CIENCIAS MÉDICASAluminium oxidevisual_art.visual_art_mediumSurgeryMedicina Oral Patología Oral y Cirugia Bucal
researchProduct

Accuracy combining different brands of implants and abutments

2013

Objective: To evaluate the vertical misfit between different brands of dental implants and prosthetic abutments, with or without mechanical torque, and to study their possible combination. Study design: Five different brands of implant were used in the study: Biofit (Castemaggiore, Italy), Bioner S.A. (Barcelona, Spain), 3i Biomet (Palm Beach, U.S.A.), BTI (Alava, Spain) and Nobel Biocare (Göteborg, Sweden), with standard 4.1 mm heads and external hexagons, and their respective machined prosthetic abutments. The implant-to- abutment fit/misfit was evaluated at four points (vestibular, lingual/palatine, mesial and distal) between implants and abutments of the same brand and different brands,…

AbutmentDentistryDental AbutmentsOdontologíaProsthesis DesignVertical fitSem micrographsProsthesis fittingDental AbutmentsClinical and Experimental DentistryProsthesis FittingCIENCIA DE LOS MATERIALES E INGENIERIA METALURGICATorqueProsthesis designGeneral DentistryProsthetic abutmentMathematicsDental Implantsbusiness.industryImplant:CIENCIAS MÉDICAS [UNESCO]Ciencias de la saludTorqueOtorhinolaryngologyCombinationUNESCO::CIENCIAS MÉDICASDentalResearch-ArticleSurgeryImplantbusiness
researchProduct

Bond strength of selected composite resin-cements to zirconium-oxide ceramic

2012

Objectives: The aim of this study was to evaluate bond strengths of zirconium-oxide (zirconia) ceramic and a selection of different composite resin cements. Study Design: 130 Lava TM cylinders were fabricated. The cylinders were sandblasted with 80 μm aluminium oxide or silica coated with CoJet Sand. Silane, and bonding agent and/or Clearfil Ceramic Primer were applied. One hundred thirty composite cement cylinders, comprising two dual-polymerizing (Variolink II and Panavia F) and two autopolymerizing (Rely X and Multilink) resins were bonded to the ceramic samples. A shear test was conducted, followed by an optical microscopy study to identify the location and type of failure, an elec…

CeramicsMaterials scienceComposite numberSurface treatmentOdontologíaDental bondingComposite ResinsDental Materialschemistry.chemical_compoundCIENCIA DE LOS MATERIALES E INGENIERIA METALURGICABiomaterials and Bioengineering in DentistryMaterials TestingCubic zirconiaCeramicComposite materialGeneral DentistryCementBond strengthShear bond strengthDental BondingSilica coating:CIENCIAS MÉDICAS [UNESCO]SilaneCiencias de la saludResin CementsOtorhinolaryngologychemistryvisual_artUNESCO::CIENCIAS MÉDICASvisual_art.visual_art_mediumZirconia ceramicsResearch-ArticleSurgeryZirconiumAdhesivePhosphate monomer
researchProduct