0000000000385574
AUTHOR
David Busquets-mataix
In vitro experimental study of bonding between aluminium oxide ceramics and resin cements
To evaluate bond strengths of different resin cements to two aluminum oxide-based ceramics. Methods: One hundred ten ceramic cylinders were produced and given four different surface treatments. Resin cement cylinders were then bonded to the ceramic cylinders using different resin cements and the bond strength was determined by shear testing to the breaking point. We were thus able to obtain results for the different combinations of porcelain, surface treatments and cements. All data was analyzed using the Kruskal-Wallis test for more than two independent samples and the Bonferroni correction applied (a=0.01). An optical microscopy study was carried out to analyze the type of failure, and an…
A novel picture for charge transport interpretation in epitaxial manganite thin films
Transport characterizations of epitaxial La0.7Sr0.3MnO3 thin films in the thickness range 5-40 nm and 25-410 K temperature interval have been accurately collected. We show that taking into account polaronic effects allows to achieve the best ever fitting of the transport curves in the whole temperature range. The Current Carriers Density Collapse picture accurately accounts for the properties variation across the metal-insulator-transition. The electron-phonon coupling parameter estimations are in a good agreement with theoretical predictions. The results promote a clear and straightforward quantitative description of the manganite films involved in charge transport device applications.
Bond strength of selected composite resin-cements to zirconium-oxide ceramic
Objectives: The aim of this study was to evaluate bond strengths of zirconium-oxide (zirconia) ceramic and a selection of different composite resin cements. Study Design: 130 Lava TM cylinders were fabricated. The cylinders were sandblasted with 80 μm aluminium oxide or silica coated with CoJet Sand. Silane, and bonding agent and/or Clearfil Ceramic Primer were applied. One hundred thirty composite cement cylinders, comprising two dual-polymerizing (Variolink II and Panavia F) and two autopolymerizing (Rely X and Multilink) resins were bonded to the ceramic samples. A shear test was conducted, followed by an optical microscopy study to identify the location and type of failure, an elec…