Near band edge and defect emissions in wurtzite Cd0.025Mg0.10Zn0.875O nanocrystals
Abstract We report on near band edge and local defects emissions in Cd0·025Mg0·10Zn0·875O (CdMgZnO) nanoparticles (NPs) as a function of temperature, where a strong temperature-dependent near-infrared emission around 1.7 eV (~730 nm) has been observed. The NPs were synthesized by a modified sol-gel method and were annealed at 750 °C after growing. The crystallographic parameters have been determined by 2-dimensional synchrotron x-ray diffraction (XRD) and conventional XRD analysis, confirming their growth within the wurtzite phase with a preferred orientation along the (101) plane and an apparent crystallite size of 52.72 ± 0.18 nm. This apparent crystallite size is consistent with the near…