Correlation between the fractal dimension of the electrode surface and the EIS of the zinc anodic dissolution for different kinds of galvanized steel
Francisco VicenteJosé Juan García-jareñoDavid Giménez-romerosubject
Working electrodeMaterials scienceMetallurgychemistry.chemical_elementZincSurface finishFractal dimensionGalvanizationCorrosionDielectric spectroscopylcsh:Chemistrysymbols.namesakechemistrylcsh:Industrial electrochemistrylcsh:QD1-999ElectrodeElectrochemistrysymbolslcsh:TP250-261description
The roughness of the working electrode is one of the factors that affects the electrochemical impedance spectroscopy (EIS) data of the zinc anodic dissolution process. The fractal dimension of digital images of shooping plate, hot dip galvanized steel, continuous hot-dipped galvanized steel and electro-galvanized steel are related with their respective EIS data. Keywords: EIS, Fractal dimension, Roughness, Galvanized steel, Corrosion
year | journal | country | edition | language |
---|---|---|---|---|
2004-02-01 | Electrochemistry Communications |