Comparing the luminescence processes of YVO4:Eu and core-shell YVO4@YF3 nanocrystals with bulk-YVO4:Eu
2017
Abstract Comparative analysis of bulk, non-coated and core-shelled nanocrystalline YVO4:Eu was performed by means of time-resolved luminescence and VUV excitation luminescence spectroscopy techniques. Nanocrystalline YVO4:Eu samples – both as-prepared and YF3 core-shelled – have been synthesized by means of a microwave-assisted synthesis in ionic liquids, which allows to obtain 10–12 nm nanoparticles with high crystallinity. The results show noticeable differences between bulk and nanocrystalline YVO4:Eu in photoluminescence experimental data, which explains by influence of the nanocrystal surface. A YF3 core-shell layer around YVO4:Eu nanoparticles partially recovers the intensity of the E…
Temperature dependence of luminescence of LiF crystals doped with different metal oxides
2020
Photoluminescence and cathodoluminescence of LiF crystals doped with different binary metal oxides were measured in the wide temperature range of 50-300 K and time interval of 10−8−10−1 s after the nanosecond electron excitation pulse. Both as-grown those and crystals irradiated by an electron beam in range of absorbed dose up to 103 Gy were studied. It is shown that spectral-kinetic characteristics of the luminescence depend on the absorbed dose (type of created/accumulated color centers), the irradiation temperature, the concentration of hydroxyl, which promotes incorporation of the MeO complex (Me: W, Ti, Fe, Li) into the crystal lattice, and the cation-dopants.
Rhodamine (B) photocatalysis under solar light on high crystalline ZnO films grown by home-made DC sputtering
2018
Abstract ZnO thin films were deposited by home-made DC sputtering of zinc target under mixed gases (Argon, Oxygen) plasma on glass substrates. Films were deposited by varying oxygen partial pressure (PO2) from 0.09 to 1.3 mbar in the deposition chamber, at a fixed substrate temperature of 100 °C. The samples were characterized by photoluminescence (PL), X-ray diffraction (XRD), optical transmissions (UV–vis), scanning electron microscopy (SEM) and electrical (Hall effect) measurements. The results indicate that by varying the oxygen pressure in the deposition chamber, the films show a precise and well defined photoluminescence emissions for each range of pressure covering almost the entire …
X-Ray studies on optical and structural properties of ZnO nanostructured thin films
2006
Abstract X-ray absorption near-edge fine structure (XANES) studies have been carried out on nanostructured ZnO thin films prepared by atmospheric pressure chemical vapour deposition (APCVD). Films have been characterized by X-ray diffraction (XRD) and optical luminescence spectroscopy exciting with laser light (PL) or X-ray (XEOL). According to XRD measurements, all the APCVD samples reveal a highly (002) oriented crystalline structure. The samples have different thickness (less than 1 μm) and show significant shifts of the PL and XEOL bands in the visible region. Zn K-edge XANES spectra were recorded using synchrotron radiation at BM08 of ESRF (France), by detecting photoluminescence yield…
Optimization of a laser ion source for $^{163}$Ho isotope separation
2019
To measure the mass of the electron neutrino, the “Electron Capture in Holmium-163” (ECHo) collaboration aims at calorimetrically measuring the spectrum following electron capture in 163Ho. The success of the ECHo experiment depends critically on the radiochemical purity of the 163Ho sample, which is ion-implanted into the calorimeters. For this, a 30 kV high transmission magnetic mass separator equipped with a resonance ionization laser ion source is used. To meet the ECHo requirements, the ion source unit was optimized with respect to its thermal characteristics and material composition by means of the finite element method thermal-electric calculations and chemical equilibrium simulation…
Low-temperature luminescence of CdI2 under synchrotron radiation
2020
Synchrotron radiation is applied to study visible and UV luminescence spectra and their excitation spectra of undoped as well as In and Sb doped cadmium iodide crystals at 10 K. The origin of principal luminescence bands and the role of impurities in the formation of emission centers are discussed. The luminescence properties have been explained based on the electronic structure of CdI2 crystals.
Assembly of microparticles by optical trapping with a photonic crystal nanocavity
2012
International audience; In this work, we report the auto-assembly experiments of micrometer sized particles by optical trapping in the evanescent field of a photonic crystal nanocavity. The nanocavity is inserted inside an optofluidic cell designed to enable the real time control of the nanoresonator transmittance as well as the real time visualization of the particles motion in the vicinity of the nanocavity. It is demonstrated that the optical trap above the cavity enables the assembly of multiple particles in respect of different stable conformations.
High pressure theoretical and experimental analysis of the bandgap of BaMoO4, PbMoO4, and CdMoO4
2019
We have investigated the origin of the bandgap of BaMoO4, PbMoO4, and CdMoO4 crystals on the basis of optical absorption spectroscopy experiments and ab initio electronic band structure, density of states, and electronic localization function calculations under high pressure. Our study provides an accurate determination of the bandgaps Eg and their pressure derivatives d E g / dP for BaMoO4 (4.43 eV, −4.4 meV/GPa), PbMoO4 (3.45 eV, −53.8 meV/GPa), and CdMoO4 (3.71 eV, −3.3 meV/GPa). The absorption edges were fitted with the Urbach exponential model which we demonstrate to be the most appropriate for thick crystals with direct bandgaps. So far, the narrowing of the bandgap of distinct PbMoO4…
Ab initio calculations of the electronic structure for Mn2+-doped YAlO3 crystals
2020
The electronic structure of Mn2+ ion substituted for the host Y atom in orthorhombic bulk YAlO3 crystals has been calculated by means of hybrid exchange-correlation functional HSE within density functional theory. The supercell approach has been used to simulate in Pbnm YAlO3 crystal the point defects, Mn-dopant and compensated the F+ center (oxygen vacancy with one trapped electron), to make unit cell neutral. Large 2 × 2 × 2 supercells of 160 atoms allow us to simulate substitutional point defect with concentration of about 3%. Mn2+ ions substituting for host Y form covalent Mn–O bonds, in opposite to the mostly ionic Y–O bond. The F center inserted to compensate the Mn2+ dopant in YAlO3 …
Positron annihilation characterization of free volume in microand macro-modified Cu0.4Co0.4Ni0.4Mn1.8O4ceramics
2016
Free volume and pore size distribution size in functional micro and macro-micro-modified Cu0.4Co0.4Ni0.4Mn1.8O4 ceramics are characterized by positron annihilation lifetime spectroscopy in comparison with Hg-porosimetry and scanning electron microscopy technique. Positron annihilation results are interpreted in terms of model implication positron trapping and ortho-positronium decaying. It is shown that free volume of positron traps are the same type for macro and micro modified Cu0.4Co0.4Ni0.4Mn1.8O4 ceramics. Classic Tao-Eldrup model in spherical approximation is used to calculation of the size of nanopores smaller than 2 nm using the ortho-positronium lifetime.