Effect of external basalt layers on durability behaviour of flax reinforced composites
2016
Abstract Aim of this work is to evaluate the influence of external layers of basalt-mat on the durability behaviour of flax reinforced epoxy composites. To this scope, long-term ageing tests were performed on two different laminates in critical environmental conditions. The first laminate, named Flax, was constituted by stacking ten layers of bidirectional flax fabrics. The second one, named Flax–Basalt, was produced by replacing two external flax layers with two layers of basalt mat for each side of the laminate. Both laminates were exposed to salt-fog environmental conditions, according to ASTM B 117 standard, for 60 days. Five samples per laminate were removed from salt-fog spray chamber…
Damage accumulation in a carbon/epoxy composite : Comparison between a multiscale model and computed tomography experimental results
2012
International audience; High-resolution computed tomography has been carried out for carbon/epoxy laminates loaded in situ to failure. The experimental data allows major damage mechanisms to be quantified in 3D, in an unambiguous and mechanically representative way, where previous experimental analysis is limited. A multi-scale model that predicts damage accumulation in tensile loaded composites is compared to the experimental analysis, to validate the underpinning assumptions within the model and overall performance. The model considers the random nature of fibre-strengths, stress transfer resulting from fibre breaks, fibre/matrix debonding and viscosity of the matrix. Assumptions within t…
Spanish Menopause Society position statement: Use of denosumab in postmenopausal women
2014
Denosumab is a new drug developed for the treatment of osteoporosis. Moreover, increasing evidences link denosumab with benefits in cancer, an area of interest for those in charge of the postmenopausal health. Denosumab has shown efficacy in the control of bone loss associated with hypogonadic states created by chemotherapy in breast and other cancers. Moreover, some studies reveal efficacy in reducing the progression of metastases. A panel of experts from the Spanish Menopause Society has met to develop usage recommendations based on the best available evidence.
The effect of dentine pre-treatment using bioglass and/or polyacrylic acid on the interfacial characteristics of resin-modified glass ionomer cements.
2018
Objective To evaluate the effect of load-cycle aging and/or 6 months artificial saliva (AS) storage on bond durability and interfacial ultramorphology of resin-modified glass ionomer cement (RMGIC) applied to dentine air-abraded using Bioglass 45S5 (BAG) with/without polyacrylic acid (PAA) conditioning.Methods RMGIC (Ionolux, VOCO) was applied onto human dentine specimens prepared with silicon-carbide abrasive paper or air-abraded with BAG with or without the use of PAA conditioning. Half of bonded-teeth were submitted to load cycling (150,000 cycles) and half immersed in deionised water for 24 h. They were cut into matchsticks and submitted immediately to microtensile bond strength (μTBS) …
Evaluation of positron-emission-tomography for visualisation of migration processes in geomaterials
2008
Abstract Positron-emission-tomography (PET) was applied for direct visualisation of solute transport in order to overcome the limitations of conventional methods for measuring advection and diffusion properties. At intervals from minutes to days the 3D-spatial distribution of the PET-tracer is determined. This spatiotemporal evolution of the tracer concentration can be used as experimental basis for clarification of the relevant transport processes, derivation of transport parameters, and model calibration. Here, 18 F and 124 I in 0.01 M carrier solution of KF and KI, respectively, have been chosen out of the limited number of available PET-tracers, primarily on account of their decay time …
Long-term fracture load of all-ceramic crowns: Effects of veneering ceramic thickness, application techniques, and cooling protocol
2020
Made available in DSpace on 2021-06-25T10:46:25Z (GMT). No. of bitstreams: 0 Previous issue date: 2020-11-01 Background: To evaluate, in vitro, the effects of the cooling protocol, application technique, and veneering ceramic thickness on the fracture resistance of ceramic crowns with Y-TZP frameworks. Material and Methods: 80 frameworks were made from zirconia by the CAD/CAM technique and divided into 8 groups (n = 10) according to the factors: “application technique” (stratified-L and pressed -P), “thickness” (1 mm and 2 mm), and “cooling protocol” (slow-S and fast-F) of the feldspathic veneering ceramic. After, all crowns were cemented over G10 preparations with resin cement (Panavia F, …
Influence of surface preparation on fracture load of resin composite-based repairs
2014
The purpose of the present study is to evaluate the fracture load of composite-based repairs to fractured zirconium oxide (Z) crowns and to ceramic-fused-to-metal (CM) crowns, comparing different mechanical surface preparation methods. A total of 75 crowns were repaired; samples then underwent dynamic loading and thermocycling. Final fracture load values for failure of the repaired crowns were measured and the type of fracture registered. Group I: CM: Surface preparation with a diamond bur + 9.5% Hydrofluoric Acid (HF) etching; Group II): CM: air-particle (Al 2 O 3 ) + 9.5% HF; Group III: CM: Silica coating (SiO 2 ); Group IV): Z: air-particle (Al 2 O 3 ) + HF 9.5%; Group V) Z: Silica coati…
Fracture resistance and failure mode of posterior fixed dental prostheses fabricated with two zirconia CAD/CAM systems.
2014
Background In recent years there has been an improvement of zirconia ceramic materials to replace posterior missing teeth. To date little in vitro studies has been carried out on the fracture resistance of zirconia veneered posterior fixed dental prostheses. This study investigated the fracture resistance and the failure mode of 3-unit zirconia-based posterior fixed dental prostheses fabricated with two CAD/CAM systems. Material and Methods Twenty posterior fixed dental prostheses were studied. Samples were randomly divided into two groups (n=10 each) according to the zirconia ceramic analyzed: Lava and Procera. Specimens were loaded until fracture under static load. Data were analyzed usin…
Fracture toughness of different monolithic zirconia upon post-sintering processes
2021
Background Surface treatments are expected to be a reason for alteration in fracture resistance of zirconia. This study evaluated the effect of post-sintering processes on the fracture toughness of different types of monolithic zirconia. Material and Methods Classical- (Cz) and high-translucent (Hz) monolithic zirconia discs (1.2 mm thickness, 14 mm in Ø) were prepared, and randomly divided for surface treatments with 1) as-glazed (AG); 2) finished and polished (FP); 3) finished, polished, and overglazed (FPOG); and 4) finished, polished, and heat-treated (FPHT) technique (n=15/group). Fracture toughness (KIC) was determined with indentation fracture toughness method at load 1 kg for AG, FP…
Post-fatigue fracture resistance of metal core crowns: press-on metal ceramic versus a conventional veneering system
2014
Background The aim of this in vitro study was to compare the mechanical failure behavior and to analyze fracture characteristics of metal ceramic crowns with two veneering systems – press-on metal (PoM) ceramic versus a conventional veneering system – subjected to static compressive loading. Material and Methods Forty-six crowns were constructed and divided into two groups according to porcelain veneer manufacture. Group A: 23 metal copings with porcelain IPS-InLine veneering (conventional metal ceramic). Group B: 23 metal copings with IPS-InLine PoM veneering porcelain. After 120,000 fatigue cycles, the crowns were axially loaded to the moment of fracture with a universal testing machine. …