Cellulose-inorganic hybrids of strongly reduced thermal conductivity

2022

Abstract The employment of atomic layer deposition and spin coating techniques for preparing inorganic-organic hybrid multilayer structures of alternating ZnO-CNC layers was explored in this study. Helium ion microscopy and X-ray reflectivity showed the superlattice formation for the nanolaminate structures and atomic force microscopy established the efficient control of the CNCs surface coverage on the Al-doped ΖnO by manipulating the concentration of the spin coating solution. Thickness characterization of the hybrid structures was performed via both ellipsometry and X-ray reflectivity and the thermal conductivity was examined by time domain thermoreflectance technique. It appears that ev…

Materials scienceSURFACEPolymers and Plastics116 Chemical sciencesHybridsFILMSchemistry.chemical_compoundThermal conductivitysinkkioksidiZinc oxideCelluloseZINC-OXIDElämmöneristysHybridCellulose nanocrystalsAluminum dopingatomikerroskasvatusDEGRADATIONNANOCOMPOSITESNANOCRYSTALSYIELDChemical engineeringchemistryThermal conductivitylämmön johtuminenNANOCELLULOSEnanoselluloosaohutkalvotCellulose
researchProduct

Salt spray fog ageing of hybrid composite/metal rivet joints for automotive applications

2017

Abstract The present experimental investigation aims to investigate the effect of salt-fog exposition on the mechanical behaviour of composite/metal riveted joints. To this aim, two kinds of joint were exposed to salt-fog environmental conditions according to ASTM B117 standard, for fifteen weeks. In particular, two composite laminates (i.e. glass fibre and carbon fibre/epoxy composites) were used as composite substrate joined with the metal substrate (i.e. aluminium alloy Al 6060). Single-lap shear tests were carried out in order to evaluate the evolution of the mechanical performances and the damage mechanisms of the riveted joints during the ageing exposition. The results evidence that t…

Materials scienceSalt-fogAluminium alloyGlass fiberComposite numberComposite02 engineering and technologyIndustrial and Manufacturing EngineeringCorrosion0203 mechanical engineeringAluminium alloyRivetComposite materialRivetingJoint (geology)Mechanical EngineeringMetallurgyHybrid jointEpoxyComposite laminates021001 nanoscience & nanotechnologyEnvironmental degradationSettore ING-IND/22 - Scienza E Tecnologia Dei Materiali020303 mechanical engineering & transportsMechanics of Materialsvisual_artCeramics and Compositesvisual_art.visual_art_mediumAluminium alloy; Composites; Environmental degradation; Hybrid joints; Riveting; Salt-fog0210 nano-technologyComposites Part B: Engineering
researchProduct

Aging resistance of bio-epoxy jute-basalt hybrid composites as novel multilayer structures for cladding

2017

Abstract Aging resistance of jute reinforced laminates is compared with two jute/basalt hybrid laminates prepared with different stacking sequences (i.e., sandwich and intercalated configuration). To this aim, composites are exposed to cyclic conditions comprising hygrothermal stress and UV radiation to promote an accelerated aging, for a period of 84 days. Specimens of each laminate are tested after 14, 28, 56 and 84 days, respectively. Quasi-static flexural tests, Charpy impact tests and dynamic mechanical tests are performed according to international ASTM and ISO standards. Furthermore, scanning electron microscopy and differential scanning calorimetry are used to evaluate the morpholog…

Materials scienceScanning electron microscopeCharpy impact testSettore ICAR/11 - Produzione Edilizia02 engineering and technology010402 general chemistry01 natural sciencesDifferential scanning calorimetryFlexural strengthComposite materialCuring (chemistry)Impact behaviourCivil and Structural EngineeringPolymer-matrix compositeEpoxy021001 nanoscience & nanotechnologyCladding (fiber optics)Accelerated agingHybrid0104 chemical sciencesEnvironmental degradationSettore ING-IND/22 - Scienza E Tecnologia Dei Materialivisual_artembryonic structuresCeramics and Compositesvisual_art.visual_art_medium0210 nano-technology
researchProduct

Initial light-induced degradation study of multicrystalline modules made from silicon material processed through different manufacturing routes

2012

The paper presents results of initial lightinduced degradation (LID) of multicrystalline silicon photovoltaic (PV) modules made of crystalline silicon from different manufacturing processes. The modules were installed within the Sunbelt, in Hyderabad, India. Current-voltage (I–V) characteristics are measured and infra-red (IR) images of the modules are taken at regular intervals. A relationship of the IV degradation with the IR images is discussed. Results from laboratory LID tests at room temperature are performed parallel to the outdoor degradation of PV modules. It was found that the total LID, measured on the module level, after the initial 40 hours is similar for both materials resulti…

Materials scienceSiliconbusiness.industryPhotovoltaic systemchemistry.chemical_elementCellular levelTemperature measurementchemistryLight inducedOptoelectronicsDegradation (geology)Power outputCrystalline siliconbusiness2012 38th IEEE Photovoltaic Specialists Conference
researchProduct

Mechanical recycling of polylactide, upgrading trends and combination of valorization techniques

2016

[EN] The upcoming introduction of polylactides in the fractions of polymer waste encourages technologists to ascertain its valorization at the best quality conditions. Mechanical recycling of PLA represents one of the most cost-effective methodologies, but the recycled materials are usually directed to downgraded applications, due to the inherent thermomechanical degradation affecting its mechanical, thermal and rheological performance. In this review, the current state of mechanical recycling of PLA is reported, with special emphasis on a multi-scale comparison among different studies. Additionally, the applications of physical and chemical upgrading strategies, as well as the chances to b…

Materials scienceSolucions polimèriquesBiopolymerPolymers and PlasticsGeneral Physics and AstronomyValorization02 engineering and technologyReview010402 general chemistryPolymer waste01 natural sciencesDegradationMaterials ChemistryForensic engineeringRecyclingProcess engineeringbusiness.industryAtomic force microscopyOrganic ChemistryTermoplàstics021001 nanoscience & nanotechnology0104 chemical sciencesUpgradingReprocessingPolylactide (PLA)MAQUINAS Y MOTORES TERMICOS0210 nano-technologybusiness
researchProduct

Relevant factors for the eco-design of polylactide/sisal biocomposites to control biodegradation in soil in an end-of-life scenario

2017

[EN] The eco-design considers the factors to prepare biocomposites under an end-of-life scenario. PLA/sisal biocomposites were obtained from amorphous polylactide and sisal loadings of 10, 20 and 30 wt% with and without coupling agent, and subjected to biodegradation in soil according to standard IS0846. Mass loss, differential scanning calorimetry and size-exclusion chromatography were used for monitoring biodegradation. A statistical factorial analysis based on the molar mass M-n, and crystallinity degree X-c pointed out the relevance and interaction of amount of fibre and use of coupling agent with the time of burial in soil., During the preparation of biocomposites, chain scission provo…

Materials scienceSolucions polimèriquesPolymers and Plastics02 engineering and technology010402 general chemistry01 natural sciencesSisalDegradationDifferential scanning calorimetryStatistical factorial analysisSize exclusion chromatographyDifferential scanning calorimetryMaterials ChemistryComposite materialSISALcomputer.programming_languageMaterials compostosTermoplàsticsBiodegradation021001 nanoscience & nanotechnologyCondensed Matter Physics0104 chemical sciencesAmorphous solidPolylactide (PLA)Natural fibreMechanics of MaterialsMAQUINAS Y MOTORES TERMICOSDegradation (geology)Biodegradation in soilBiocomposite0210 nano-technologycomputerBiocompositeDesign of experiments
researchProduct

Polylactide-based self-reinforced composites biodegradation: Individual and combined influence of temperature, water and compost

2018

[EN] Self-reinforced polymer composites (SRCs) are proposed as a suitable alternative for composite development, based in the combination of a polymeric matrix and a polymeric fibre made of the same polymer. SRCs based in polylactide (PLA) could be fully biodegradable and their valorisation routes could presumably be assimilated to those for neat PEA. In this sense, the aim of this study was to develop new self-reinforced PLA-based composites and ascertain their biodegradability. For this purpose, PLA-based SRCs were obtained through a thermo-compression procedure and their biodegradability corroborated under standard conditions (ISO 20200). Moreover, a deep study of the effect of the diffe…

Materials scienceSolucions polimèriquesPolymers and PlasticsComposite number02 engineering and technologyengineering.material010402 general chemistry01 natural sciencesSelf reinforcedCIENCIA DE LOS MATERIALES E INGENIERIA METALURGICAMaterials ChemistryComposite materialchemistry.chemical_classificationMolar massCompostCompostingINGENIERIA DE LOS PROCESOS DE FABRICACIONPolymerBiodegradationCiència dels materials021001 nanoscience & nanotechnologyCondensed Matter PhysicsHydrothermal degradation0104 chemical sciencesSelf-reinforced composites (SRCs)chemistryPolylactide (PLA)Mechanics of MaterialsThermal degradationMAQUINAS Y MOTORES TERMICOSengineeringBiodegradationDegradation (geology)Valorisation0210 nano-technology
researchProduct

Grafting of Maleic Anhydride onto Isotactic Polypropylene in the Presence of Supercritical Carbon Dioxide as a Solvent and Swelling Fluid

2004

Grafting of maleic anhydride (MA) onto isotactic polypropylene (iPP) was carried out by thermal decomposition of dicumylperoxide (DCP) using supercritical carbon dioxide (scCO2) as a solvent and swelling fluid. Provided that the initial concentration of anhydride dissolved in scCO2 is higher than 1% w/w, the grafting occurs without significant molecular weight modification of the polymer, and with a proper selection of the operative conditions, a grafting level higher than 0.5% w/w with respect to the polymer mass was obtained. The amount of grafted MA was determined by FT-IR spectroscopy and polymer degradation was monitored by dynamic mechanical tests in the melt state. The effect of MA a…

Materials scienceSupercritical carbon dioxidePolymers and PlasticsOrganic ChemistryMaleic anhydridepolypropylene maleic anhydride polymerGraftingInorganic Chemistrychemistry.chemical_compoundPolymer degradationchemistryChemical engineeringTacticityPolymer chemistryMaterials ChemistrymedicinePolymer blendSwellingmedicine.symptomMelt flow indexMacromolecules
researchProduct

Protection of high-density polyethylene-silicon composites from ultraviolet-visible photodegradation

2017

[EN] The extent of the ultraviolet¿visible (UV¿vis) photoirradiation effect on high-density polyethylene (HDPE) and HDPE¿sili-con (Si) composites is reported in terms of the addition of Si microparticles at contents of 0.1, 1, and 5 wt %. A standard acceleratedUV-vis exposure was applied over 2750 h, corresponding to 22 months in Florida. Thermogravimetry, differential scanning calorimetry,and Fourier transform infrared spectroscopy were used as reliable techniques for monitoring the quality of the HDPE-Si composites. Theincreasing addition of Si microparticles delayed the photodegradation of the HDPE¿Si composites. Because of their strong light-scattering effects, Si microparticles blocked…

Materials scienceThermal propertiesPolymers and PlasticsSiliconComposite numberDifferential scanning calorimetry (DSC)chemistry.chemical_element02 engineering and technology010402 general chemistry01 natural sciencesElectron Microscopy Service of the UPVchemistry.chemical_compoundDegradationDifferential scanning calorimetryMaterials ChemistryFourier transform infrared spectroscopyComposite materialPhotodegradationMaterials compostosThermogravimetric analysis (TGA)TermoplàsticsGeneral ChemistryPolyolefinsPolyethylene021001 nanoscience & nanotechnology0104 chemical sciencesSurfaces Coatings and FilmsThermogravimetrychemistryMAQUINAS Y MOTORES TERMICOSHigh-density polyethylene0210 nano-technology
researchProduct

Influence of sol counter-ions on the visible light induced photocatalytic behaviour of TiO2 nanoparticles

2014

Titanium dioxide (TiO2) nanoparticles are attracting increasing interest because of their superior photocatalytic and antibacterial properties. Here, aqueous titanium oxy-hydroxide sols were made, using a green synthesis method, from the controlled hydrolysis/peptisation of titanium isopropoxide. Three different mineral acids were used to peptise the sol (HNO3, HBr and HCl), and provide counter-ions. The influence of nitrate or halide sol counter-ions on size distributions of the starting sols were measured via photon correlation spectroscopy (PCS). Semi-quantitative phase composition analysis (QPA), on the gels thermally treated at 450 and 600 degrees C, was carried out via Rietveld refine…

Materials scienceTiO2 photocatalysis self-cleaning additive building materialInorganic chemistryGARNET YAG FIBERSSettore ICAR/10 - Architettura TecnicaHalidechemistry.chemical_elementCatalysisFERRITE FIBERSchemistry.chemical_compoundHETEROGENEOUS PHOTOCATALYSISORGANIC CONTAMINANTSTitanium isopropoxideGREEN CHEMISTRYSettore CHIM/03 - Chimica Generale e InorganicaTITANIUM-DIOXIDEBrookiteRietveld refinementSettore CHIM/07 - Fondamenti Chimici delle TecnologieOPTICAL-PROPERTIESDEGRADATIONANATASE-RUTILE TRANSFORMATIONSettore ING-IND/22 - Scienza E Tecnologia Dei MaterialichemistryRutilevisual_artTitanium dioxidevisual_art.visual_art_mediumPhotocatalysisGEL PRECURSORTitanium
researchProduct