Search results for "Optical Fibers"
showing 10 items of 107 documents
Improved All-Fiber Acousto-Optic Tunable Bandpass Filter
2017
An all-fiber acousto-optic tunable bandpass filter based on a 1.185-mm long coreless core mode blocker is reported. Experimental results demonstrate a minimal insertion loss of 1.2 dB at the optical resonant wavelength of 1527.7 nm with 3-dB optical bandwidth of 0.83 nm. The optimization of the device takes into account the attenuation of the acoustic wave and leads to an asymmetric configuration in which the coupling section is shorter than the recoupling part. Under the effect of a standing flexural wave the device can be operated as a bandpass modulator. The device exhibits a maximum modulation depth of 28%, 4 dB of insertion loss and 0.97 nm of optical bandwidth at 4.774 MHz.
Mid-infrared 2000-nm bandwidth supercontinuum generation in suspended-core microstructured Sulfide and Tellurite optical fibers
2012
International audience; In this work, we report the experimental observation of supercontinua generation in two kinds of suspended-core microstructured soft-glass optical fibers. Low loss, highly nonlinear, tellurite and As2S3 chalcogenide fibers have been fabricated and pumped close to their zero-dispersion wavelength in the femtosecond regime by means of an optical parametric oscillator pumped by a Ti:Sapphire laser. When coupled into the fibers, the femtosecond pulses result in 2000-nm bandwidth supercontinua reaching the Mid-Infrared region and extending from 750 nm to 2.8 mu m in tellurite fibers and 1 mu m to 3.2 mu m in chalcogenide fibers, respectively.
Ternary and quaternary Ge-S-Se-Sb-Te amorphous chalcogenide thin films for mid-infrared applications
2017
International audience; Chalcogenide materials exhibit a unique portfolio of properties which has led to their wide use for nonvolatile memory applications such as optical storage (CD-RW and DVD-RAM), Conductive Bridging Random Access Memory or Phase Change Random Access Memory (PCRAM). More recently, thanks to huge electronic nonlinearities under electrical field application, chalcogenide glasses are considered as most promising materials to be used as Ovonic Threshold Switching (OTS) selectors [1]. Besides, thanks to high transparency window in the infrared range and large optical nonlinearities [2], chalcogenide alloys offer the opportunity of development of innovative mid-infrared (MIR)…
Time-domain fiber laser hydrogen sensor.
2004
We report a novel scheme for a fiber-optic hydrogen sensor based on an erbium-doped fiber laser with a palladium-coated tapered fiber within the laser cavity. The tapered fiber acts as a hydrogen-sensing element. When the sensing element is exposed to a hydrogen atmosphere, its attenuation decreases, changing the cavity losses and leading to a modification of the laser transient. The hydrogen concentration is obtained by simple measurement of the buildup time of the laser. This technique translates the measurement of hydrogen concentration into the time domain, and it can be extended to many intensity-based fiber sensors. Relative variations in the buildup time of up to 55% at an increase o…
Dynamic control of the operation regimes of a mode-locked fiber laser based on intracavity polarizing fibers: experimental and theoretical validation.
2012
[EN] An intracavity polarizing fiber is proposed to control the emission regime of a passively mode-locked fiber laser. Stable operation in self-starting high and low dispersion soliton mode-locking and 100 GHz multiwavelength regimes is demonstrated through numerical simulations and experimental validation. Mode-locking stability is ensured by a saturable absorber in the ring cavity. The effective selection of operation regime is dynamically carried out by controlling the intracavity polarization state.
Suspended core tellurite glass optical fibers for infrared supercontinuum generation
2011
International audience; We report the fabrication and characterization of tellurite TeO(2)-ZnO-Na(2)O (TZN) microstructured suspended core optical fibers (MOFs). These fibers are designed for infrared supercontinuum generation with zero dispersion wavelength (ZDW) at 1.451 mu m. The measured losses at this wavelength are approximately 6 dB/m for a MOF with a 2.2 mu m diameter core. The effective area of a particular fiber is 3.5 mu m(2) and the nonlinear coefficient is calculated to be 437 W(-1)km(-1). By pumping a 20 cm long fiber at 1.56 mu m with a sub-nj femtosecond laser source, we generate a supercontinuum (SC) spanning over 800 nm in the 1-2 mu m wavelength range.
Chalcogenide glass hollow core photonic crystal fibers
2010
International audience; We report the first hollow core photonic crystal fibers (HC PCF) in chalcogenide glass. To design the required HC PCF profiles for such high index glass, we use both band diagram analysis to define the required photonic bandgap and numerical simulations of finite size HC PCFs to compute the guiding losses. The material losses have also been taken into account to compute the overall losses of the HC PCF profiles. These fibers were fabricated by the stack and draw technique from Te20As30Se50 (TAS) glass. The fibers we drew in this work are composed of six rings of holes and regular microstructures. Two profiles are presented, one is known as a kagome lattice and the ot…
Tellurites fibers for infrared supercontinuum sources : opto-geometric profiles and extrinsic absorptions management
2016
This PhD thesis work focuses on the synthesis and purification of vitreous materials used for the development of waveguides with varied profiles, dedicated to supercontinuum (SC) generation between 1 and 5 μm.Concerning the purification of tellurite glasses, several leads were followed, but best results are obtained for the purification of the TeO2-ZnO-Na2O glassy system by the means of zinc fluoride. Attenuation measurements performed on several meter-long single-index fiber samples reveal the nearly complete elimination of water-related absorptions between 3 and 4 μm (OH ions concentration lower than 1 ppm mass.). Such water-purified glasses were firstly dedicated to microstructured optic…
Fibres optiques à coeur supendu en verre d'oxyde de tellure et génération d'effets non linéaires dans l'infrarouge au-delà de 2 microns
2012
The work reported in this thesis deals with the fabrication of suspended core tellurite microstructured optical fibers (MOFs) for supercontinuum generation beyond 2 µm. In order to reach our aim, we first studied thermal and optical properties of TeO2-ZnO-R2O and TeO2-WO3-R2O (where R = Li, Na and K) glasses. The glass 80TeO2-10ZnO-10Na2O (molar %) has been chosen in order to make MOFs for characterization of the generated non linear optical effects. Synthesis performed under dry and oxidative atmosphere allowed us to reduce the hydroxyl groups concentration by a factor of 30 compared to fabrication in air atmosphere. Use of dehydrating agents (ZnF2 and TeCl4) allowed to reduce again the OH…
Polarization Modulation Instability in All-Normal Dispersion Microstructured Optical Fibers With Quasi-Continuous Pump
2019
We report the experimental observation of the polarization modulation instability (PMI) effect in all-normal dispersion (ANDi) microstructured optical fibers (MOFs) with quasi-continuous pumping. The small unintentional birefringence (~10-5), that any realistic non-polarization maintaining MOF exhibits, contributes to this nonlinear effect. PMI can produce two sidebands whose polarization state is orthogonal to the polarization of the pump. In this work, only one type of PMI process is observed, i.e., when the pump is polarized along the slow axis of the fiber and sidebands are generated in the fast axis mode. This PMI process was studied experimentally in two ANDi fibers with different dis…