A comparative study on the compatibility of liquid lead–gold eutectic and liquid lead–bismuth eutectic with T91 and SS 316LN steels
2012
Abstract Liquid lead–gold eutectic (LGE) is considered as a potential target material for high power spallation sources. In the present work, the corrosion effects of LGE on T91 and SS 316LN steels have been investigated in comparison with that of liquid lead–bismuth eutectic (LBE) under the same testing conditions. Two tests were conducted at 400 °C for 1800 h and at 450 °C for 1300 h, in which specimens of the two steels were exposed to 1 m/s flowing LGE and LBE. Surface inspections showed that the specimens underwent a mixed corrosion mode of dissolution and oxidation. The results obtained from the SS 316LN specimens are very interesting. Firstly, EDX (electron energy dispersion X-ray sp…
The n_TOF facility: Neutron beams for challenging future measurements at CERN
2016
The CERN n TOF neutron beam facility is characterized by a very high instantaneous neutron flux, excellent TOF resolution at the 185 m long flight path (EAR-1), low intrinsic background and coverage of a wide range of neutron energies, from thermal to a few GeV. These characteristics provide a unique possibility to perform high-accuracy measurements of neutron-induced reaction cross-sections and angular distributions of interest for fundamental and applied Nuclear Physics. Since 2001, the n TOF Collaboration has collected a wealth of high quality nuclear data relevant for nuclear astrophysics, nuclear reactor technology, nuclear medicine, etc. The overall efficiency of the experimental prog…
Turbulence model effect on heat exchange characteristics through the neutron beam window for European spallation source
2011
PurposeThe purpose of this paper is to compare k‐ω shear‐stress transport (SST) and large eddy simulation (LES) turbulence model application effect on numerical computation of flow pattern and heat exchange characteristics through the neutron beam window region for European spallation source setup model.Design/methodology/approachTransient hydrodynamic and thermal calculations with appropriate heat sources are performed using both turbulence models and typical discrepancies in flow and thermal patterns are discussed, as well as, simulation results are qualitatively compared with experimental data for heat transfer coefficient distribution α at the window surface.FindingsContribution of grea…
Study of exotic decay of Cs isotope close to the proton drip line
2020
6 pags., 6 figs. -- 27th International Nuclear Physics Conference (INPC2019) 29 July - 2 August 2019, Glasgow, UK
Depassivation Experiments by Laser‐Pulse‐Induced Spallation
1992
Depassivation experiments have been conducted by applying a technique developed for adhesion tests. A laser-pulse-induced spallation of the passive film is induced in situ without any contact between the laser beam and the passive film. The depassivation is controlled by the short pressures induced at the metal-film interface. The interfacial stresses at the metal-film interface could be studied by this technique
A comparison between the chemical behaviour of lead-gold and lead-bismuth eutectics towards 316L stainless steel
2013
Radiochimica acta, 101 (10)
The effect of rare earths deposited on steel surfaces, by different processes (sol/gel, electrophoresis, OMCVD), on high temperature corrosion behavi…
1993
Abstract In this paper, different methods of rare earth oxides deposition on the surface of AISI 304 steel are described: sol/gel, electrophoresis in aqueous or organic medium, OMCVD of rare earth β-diketonates. After the deposition, all the samples were reheated. This treatment was absolutely essential for a strengthening effect of the protective oxide scale. Oxidation of coated and non-coated samples was performed under isothermal and cyclic conditions. The effect of rare earth deposition is significant in isothermal conditions. However, in thermal cyclic conditions, the effect of a rare earth deposited on surface is spectacular. Scale spallation is then completely avoided under the chose…
Simulation of H- ion source extraction systems for the Spallation Neutron Source with Ion Beam Simulator.
2012
A three-dimensional ion optical code IBSimu, which is being developed at the University of Jyväskylä, features positive and negative ion plasma extraction models and self-consistent space charge calculation. The code has been utilized for modeling the existing extraction system of the H(-) ion source of the Spallation Neutron Source. Simulation results are in good agreement with experimental data. A high-current extraction system with downstream electron dumping at intermediate energy has been designed. According to the simulations it provides lower emittance compared to the baseline system at H(-) currents exceeding 40 mA. A magnetic low energy beam transport section consisting of two sole…
Influence of the mode of introduction of a reactive element on the high temperature oxidation behavior of an alumina-forming alloy. Part I: Isotherma…
2004
Several routes of yttrium introduction were applied to test the high temperature oxidation performance of a FeCrAl alloy. Isothermal oxidation tests were described in a previous paper (Part I of this paper in this journal, 2004, 55, 352). Cyclic oxidation tests were performed in air under atmospheric pressure on blank specimens, Y 2 O 3 sol-gel coated-, Y 2 O 3 metal-organic chemical vapor deposited (MOCVD)-, yttrium ion implanted-alloys, as well as on a steel containing 0.1 wt.% of yttrium as an alloying element. For the 20 hours cycles, all the samples, except FeCrAl-0.1Y, exhibit weight losses after a few cycles, indicating drastic spallation of the oxide scales. The MOCVD coated specime…
A pulsed laser technique for an evaluation of the spall resistance of sputtered oxide films: diagnostic by interferometric probing
1998
Abstract A pulsed laser technique, based on conventional laser acoustics testing, has been developed to define the spall resistance of sputtered oxide films on a metallic target. Direct irradiation of the coated side of the sample generates an acoustic source at the inner film–metal interface. A model of the laser-induced epicentral displacements at the opposite side that takes into account the confining effect of the coating has been proposed to evaluate the critical laser irradiance corresponding to progressive damages at the inner film–metal interface, i.e. interface delamination, film spallation and film expulsion, respectively. The behavior of Al 2 O 3 and ZrO 2 films deposited by PVD …