Microbeam SEE Analysis of MIM Capacitors for GaN Amplifiers
Broad-beam and microbeam single-event effect tests were performed on metal–insulator–metal capacitors with three different thicknesses of silicon nitride (Si3N4) dielectric insulator: 250, 500, and 750 nm. The broad-beam tests indicated that the devices with the thicker, 500- and 750-nm dielectric did not have a greater breakdown voltage. The surrounding structures of the capacitor were suspected to be a possible cause. Microbeam techniques made it possible to localize the failure location for the 500- and 750-nm devices. The failure occurs in the air bridge structure connected to the top capacitor plate, which can therefore be considered as an edge effect, while for the 250-nm devices, the…