6533b86efe1ef96bd12ccab5

RESEARCH PRODUCT

Polar phonons in relaxor ferroelectric 0.2PSN-0.4PMN-0.4PZN

Jan MacutkevicS. KambaKarlis BormanisJ. BanysAndris SternbergAlexej Pashkin

subject

Materials scienceCondensed matter physicsPhononInfraredGeneral Physics and AstronomyAtmospheric temperature rangesymbols.namesakeFourier transformReflection (mathematics)visual_artPercolationsymbolsvisual_art.visual_art_mediumCeramicBurns temperature

description

Relaxor ferroelectrics 0-2PbSc(1/2)Nb(1/2)O(3) - 0.4PbMg(1/3)Nb(2/3)O(3)-0.4PbZn(1/3)Nb(2/3)O(3) ceramics were studied by means of the Fourier transform infrared reflection and THz transmission spectroscopy in the temperature range of 20-500 K. On heating from low temperatures, the A(1) component of the strongly split TO1 mode softens towards the Burns temperature, but the softening ceases near 400 K, which could be a signature of polar cluster percolation temperature.

http://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcAuth=ORCID&SrcApp=OrcidOrg&DestLinkType=FullRecord&DestApp=WOS_CPL&KeyUT=WOS:000254351000021&KeyUID=WOS:000254351000021